A sewage treatment method and sewage technology, which are applied in water/sewage treatment, sludge treatment, biological water/sewage treatment, etc., can solve the problems of complicated sewage treatment process and low purification efficiency, achieve clear and transparent water body, and improve the purification effect. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0045] In an embodiment of the present invention, the preparation method of the polyacrylic acid-modified rectorite comprises the following steps:
[0046] 1) Add 800-1500 parts by weight of water to 80-120 parts by weight of rectorite, and stir at 30-50° C. for 15-24 hours to obtain a mixed solution;
[0047] 2) Add 1 to 3 parts by weight of dopamine hydrochloride to the mixed solution obtained in step 1), and stir at 40 to 60° C. for 24 to 48 hours to obtain dopamine hydrochloride modified rectorite;
[0048] 3) adding 10-20 parts by weight of polyacrylic acid to the dopamine hydrochloride-modified rectorite obtained in step 2), and stirring at 60-80° C. for 24-48 hours to obtain a semi-finished product of polyacrylic acid-modified rectorite;
[0049] 4) cooling, filtering, and drying the semi-finished polyacrylic acid-modified rectorite obtained in step 3), that is, the obtained polyacrylic acid-modified rectorite.
[0050] The purpose of modifying the rectorite with dopam...
Embodiment 1
[0072] Add 800g of water to 120g of rectorite, stir at 30°C for 15h to obtain a mixed solution; add 1g of dopamine hydrochloride to the mixed solution, and stir at 40°C for 48h to obtain dopamine hydrochloride modified rectorite; Add 20g of polyacrylic acid to the rectorite modified by dopamine hydrochloride, and stir at 80°C for 24h to obtain a semi-finished product of polyacrylic acid modified rectorite; the semi-finished product of polyacrylic acid modified rectorite is cooled, filtered, and dried. That is, the obtained polyacrylic acid-modified rectorite.
[0073] Mix 5 parts by weight of Rhodococcus erythropolis and 10 parts by weight of acetic acid, then add 80 parts by weight of water, and keep warm for 3 hours at 60°C to obtain the first material; add 40 parts by weight of Potato starch was stirred at 50°C for 3h to obtain a second material; then 50 parts by weight of polyacrylic acid-modified rectorite was added to the second material, and stirred at 60°C for 4h to ob...
Embodiment 2
[0075] Add 1500g of water to 80g of rectorite, stir at 50°C for 24h to obtain a mixed solution; add 3g of dopamine hydrochloride to the mixed solution, and stir at 60°C for 24h to obtain dopamine hydrochloride modified rectorite; Add 10g of polyacrylic acid to the rectorite modified by dopamine hydrochloride, stir at 60°C for 48h to obtain a semi-finished product of polyacrylic acid modified rectorite; cool, filter and dry the semi-finished product of polyacrylic acid modified rectorite, That is, the obtained polyacrylic acid-modified rectorite.
[0076] Mix 1 part by weight of Rhodococcus erythropolis and 40 parts by weight of acetic acid, then add 75 parts by weight of water, and keep warm at 65°C for 2 hours to obtain the first material; add 25 parts by weight of Potato starch was stirred at 55°C for 4h to obtain a second material; then 30 parts by weight of polyacrylic acid-modified rectorite was added to the second material, and stirred at 70°C for 3h to obtain a semi-fin...
PUM