Solar cell piece welding strip automatic cleaning and flux smearing method and device
A solar cell, automatic cleaning technology, applied to the device, auxiliary device, cleaning method and utensils for coating liquid on the surface, etc., can solve the problems such as easy to produce cracks and cracks, easy to corrode mechanical devices, easy to be polluted, etc. , to reduce the influence of the battery, the welding effect is firm and the welding defect rate is reduced
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0033] 1. Lay the welding strips according to the path, specifically, multiple welding strips (depending on the number of grid lines of the battery sheet, including 3 grids, 4 grids, 5 grids, etc.) in order to pass around the right side of the middle of the box in a strip shape Soldering ribbon inlet, cleaning cotton in the box cover, right short rod fixed pulley V-shaped groove, flux container box cover right square hole, long rod fixed pulley V-shaped groove, flux container box cover left square hole, The left short rod fixes the V-shaped groove of the pulley, the drying chamber, and the strip-shaped welding ribbon outlet on the left side of the middle part of the box body.
[0034] 2. Tighten the locking mechanism of the cleaning device so that the welding ribbon has sufficient friction when passing through the cleaning cotton; inject alcohol to ensure that the cleaning cotton is wet to clean the adhesion of the welding ribbon.
[0035] 3. Adjust the length of the long pole...
Embodiment 2
[0041] The process is the same as in Example 1, except that no alcohol cleaning agent is added to the ribbon cleaning device, the heating power of the drying device is controlled at a temperature of 50° C., and the flow velocity is at 4 levels (equivalent to 3 m / s). Start the stringer and count the defect rates of cell welding. The total defect rate of cell welding is 0.4%, the rate of virtual welding and open welding is 0.18%, and the rate of splinters and hidden cracks is 0.20%.
Embodiment 3
[0043] The process is the same as in Example 2, except that the support of the ribbon cleaning device is not fastened (the device has no cleaning function), the heating power of the drying device is controlled at a temperature of 40°C, and the flow velocity is set at 5 levels (equivalent to 1m / s). Start the stringer device, and count the defect rates of cell welding. The total defect rate of cell welding is 0.55%, the rate of virtual welding and open welding is 0.20%, and the rate of splinters and hidden cracks is 0.34%.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com