Handling method for intensified leaching-extracting recovery of iron and chromium with chromium slag and mixed acid
A technology of enhanced leaching and treatment method, which is applied in the field of chromium slag mixed acid enhanced leaching-extraction and recovery of iron and chromium, which can solve unrealized problems and achieve the effect of reducing yellowing and high purity
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0041] A certain chromium slag contains 3.12% of total chromium and 0.85% of hexavalent chromium. Add 6L of water, 200ml of concentrated sulfuric acid and 1500ml of hydrochloric acid to 1kg of chromium slag. After reacting at 60-80℃ for 60min, add 40g of glucose and reduce it at 80-90℃ for 3h. , then add polyether 15g and stir for 30min, stop stirring, let stand for 24h and then filter to obtain 3.56g / L of total chromium, 0.5mg / L of hexavalent chromium, and 8.7g / L of iron. Silicon dioxide 0.4g / L leaching solution. The remaining slag has a dry weight of 950g and contains 0.23% of total chromium. The washed slag is dissolved and tested according to the "Identification Standard for Hazardous Waste-Leach Toxicity Identification" (GB5085.3-2007), HJ687-2014 Alkali Digestion Method, and the water solubility The content of hexavalent chromium complies with the second-level discharge standard of "chromium salt industrial pollutant discharge standard", and the water-soluble hexavalent ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com