A cleanliness and turbine technology, applied in the field of lubricating oil, can solve the problems of unsuitability for combined cycle turbines, disassembly and cleaning, high maintenance costs, short service life of turbine oil, etc., to achieve excellent emulsification resistance, superior low temperature stability, and extended The effect of service life
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
no. 1 Embodiment
[0026] A preparation method of high-cleanliness extreme-pressure turbine oil, comprising the steps of:
[0027] Step 1: prepare synthetic base oil according to the weight ratio of PAO4:PAO10:diester=36:25:33;
[0028] Step 2: Weigh each component by the following parts by weight:
[0029]
[0030]
[0031] Step 3: Add synthetic base oil into the reactor, stir and heat to 65°C;
[0032] Step 4: Put pour point depressant and viscosity index improver into the reactor once more, stir at 300r / min for 30 minutes,
[0033] Step 5: Continue to put high-temperature antioxidant, detergent and dispersant, friction modifier and extreme pressure anti-wear agent into the reactor, and stir at 350r / min for 90 minutes;
[0034] Step 6: Finally, put the antirust agent into the reaction kettle and stir for 90 minutes at a speed of 150r / min;
[0035] Step 7: Transfer the materials in the reactor to the storage tank and let it stand for 120 minutes to obtain the turbine oil.
[0036] The...
no. 2 Embodiment
[0039] A preparation method of high-cleanliness extreme-pressure turbine oil, comprising the steps of:
[0040] Step 1: prepare synthetic base oil according to the weight ratio of PAO4:PAO10:diester=38:26:33;
[0041] Step 2: Weigh each component by the following parts by weight:
[0042]
[0043]
[0044] Step 3: Add synthetic base oil into the reactor, stir and heat to 65°C;
[0045] Step 4: Put pour point depressant and viscosity index improver into the reactor once more, stir at 300r / min for 30 minutes,
[0046] Step 5: Continue to put high-temperature antioxidant, detergent and dispersant, friction modifier and extreme pressure anti-wear agent into the reactor, and stir at 350r / min for 90 minutes;
[0047] Step 6: Finally, put the antirust agent into the reaction kettle and stir for 90 minutes at a speed of 150r / min;
[0048] Step 7: Transfer the materials in the reactor to the storage tank and let it stand for 120 minutes to obtain the turbine oil.
[0049] The...
no. 3 Embodiment
[0051] A preparation method of high-cleanliness extreme-pressure turbine oil, comprising the steps of:
[0052] Step 1: prepare synthetic base oil according to the weight ratio of PAO4:PAO10:diester=36:27:33;
[0053] Step 2: Weigh each component by the following parts by weight:
[0054]
[0055] Step 3: Add synthetic base oil into the reactor, stir and heat to 65°C;
[0056] Step 4: Put pour point depressant and viscosity index improver into the reactor once more, stir at 300r / min for 30 minutes,
[0057] Step 5: Continue to put high-temperature antioxidant, detergent and dispersant, friction modifier and extreme pressure anti-wear agent into the reactor, and stir at 350r / min for 90 minutes;
[0058] Step 6: Finally, put the antirust agent into the reaction kettle and stir for 90 minutes at a speed of 150r / min;
[0059] Step 7: Transfer the materials in the reactor to the storage tank and let it stand for 120 minutes to obtain the turbine oil.
[0060] The turbine oil...
PUM

Abstract
Description
Claims
Application Information

- Generate Ideas
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com