Waterborne wood floor paint for roller painting of containers

A container and floor paint technology, applied in coatings, biocide-containing paints, anti-fouling/underwater paints, etc., can solve problems such as unsatisfactory, no container floor paint roller coating, poor defoaming performance, etc. question

Active Publication Date: 2017-09-15
广东伊思曼新材料科技股份有限公司
View PDF6 Cites 8 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0004] In the prior art, there are also many patents or documents disclosing some water-based wood coatings and their production methods, but the coating effects in these patents mostly only meet some basic physical performance indicators of environmental protection performance and paint film, and the construction method is generally only Ordinary brushing or spraying, if it is used for roller coating, the defoaming property is poor,

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • Waterborne wood floor paint for roller painting of containers
  • Waterborne wood floor paint for roller painting of containers
  • Waterborne wood floor paint for roller painting of containers

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0099] The water-based wood floor paint for container roller coating provided in this example includes component A, component B and water. The mass ratio of component A, component B and water is 100:5:20. The specific formula It can be formulated as follows (mass percentage):

[0100] A component:

[0101] Composite modified self-crosslinking acrylic polymer 63%

[0102] Composite modified wear-resistant polymer 21%

[0103] Defoamer 0.2%

[0104] Dispersant 0.2%

[0105] Water-based matting agent 1.2%

[0106] Thickener 0.5%

[0107] Leveling agent 0.4%

[0108] Smoothing and anti-blocking aid 0.3%

[0109] Anti-mildew fungicide 0.5%

[0110] Water 12.7%,

[0111] Component B

[0112] Multifunctional Aziridine Crosslinker 30%

[0113] Polycarbodiimide crosslinker 30%

[0114] water 40%,

[0115] The composite modified self-crosslinking acrylic polymer in component A is composed of the following components in mass percentage: 50% of organic silicon modified self-c...

Embodiment 2

[0141] The water-based wood floor paint for container roller coating provided in this example includes component A, component B and water. The mass ratio of component A, component B and water is 100:8:20. The specific formula It can be formulated as follows (mass percentage):

[0142] A component:

[0143] Composite modified self-crosslinking acrylic polymer 56%

[0144] Composite modified wear-resistant polymer 28%

[0145] Defoamer 0.4%

[0146] Dispersant 0.4%

[0147] Water-based matting agent 0.8%

[0148] Thickener 0.3%

[0149] Leveling agent 0.2%

[0150] Smoothing and anti-blocking aid 0.4%

[0151] Anti-mildew fungicide 0.3%

[0152] Water 13.2%,

[0153] B component

[0154] Multifunctional Aziridine Crosslinker 20%

[0155] Polycarbodiimide crosslinker 30%

[0156] water 50%

[0157] The sum of the mass percentages of each raw material is 100%;

[0158] The composite modified self-crosslinking acrylic polymer in component A is composed of the followin...

Embodiment 3

[0169] The water-based wood floor paint for container roller coating provided in this example includes component A, component B and water. The mass ratio of component A, component B and water is 100:10:20. The specific formula It can be formulated as follows (mass percentage):

[0170] A component:

[0171] Composite modified self-crosslinking acrylic polymer 58%

[0172] Composite modified wear-resistant polymer 26%

[0173] Defoamer 0.3%

[0174] Dispersant 0.3%

[0175] Water-based matting agent 1%

[0176] Thickener 0.4%

[0177] Leveling agent 0.3%

[0178] Smoothing and anti-blocking aid 0.3%

[0179] Anti-mildew fungicide 0.4%

[0180] Water 13%

[0181] Component B

[0182] Multifunctional Aziridine Crosslinker 25%

[0183] Polycarbodiimide crosslinker 25%

[0184] water 50%

[0185] The sum of the mass percentages of each raw material is 100%;

[0186] The composite modified self-crosslinking acrylic polymer in component A is composed of the following co...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses waterborne wood floor paint for roller painting of containers. The waterborne wood floor paint comprises a first component, a second component and water in a mass ratio of 100:5-10:10-20. The first component is prepared from a composite modified self-crosslinking acrylic polymer, a composite modified wear-proof polymer, an anti-foaming agent, a dispersing agent, a waterborne flatting agent, a thickening agent, a leveling agent, smoothening and anti-adhesion additives, an anti-mildew bactericide and the balance water. The second component is prepared from a composite modified cross-linking agent and water. The waterborne wood floor paint for roller painting of the containers is great in effect, environmental friendly, especially suitable for roller painting, excellent in anti-foaming performance and abrasion resistance, high in hardness, excellent in anti-cracking performance under cold and hot conditions, anti-adhesion performance at a high temperature and water resistance, quick in drying, moderate in cost, easy in construction and high in efficiency.

Description

technical field [0001] The invention belongs to the technical field of water-based wood coatings, in particular to a water-based wood floor paint for container roller coating and a preparation method thereof. Background technique [0002] As a decorative material, wood floor paint has higher and higher decorative requirements and environmental performance. As a wood floor decoration material for containers, the traditional two-component solvent-based PU wood floor paint has different product formulas and processes. It is very mature, and its product performance can also meet higher demands. It is mainly manifested in the application of roller coating, which is easy to defoam, good adhesion and fullness, high hardness can reach between H-2H, water resistance, high temperature resistance and back adhesion It has good alcohol and alcohol resistance and is not easy to lose luster. However, because it contains a large amount of volatile organic compounds (VOC), it will cause cert...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
IPC IPC(8): C09D133/00C09D175/04C09D5/14C09D7/12
CPCC08L2205/035C09D5/14C09D133/00C08L75/04C08L79/00C08K13/02C08K5/3412C08K3/40C08K3/36
Inventor 丘子范冯星俊刘光勇
Owner 广东伊思曼新材料科技股份有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products