Embodiment 1
[0041] 10 parts of peanut oil,
[0042] Rosin 25 parts,
[0043] Vaseline 15 parts,
[0044] Kaolin 15 parts,
[0045] Filling 30 parts,
[0046] 1 part paint,
[0047] Phosphor powder 1 part;
[0048] Wherein, the filler includes calcium carbonate, alumina and silicon dioxide; the fineness of the filler is 200 mesh-300 mesh; the fluorescent powder includes: talcum powder 30-40% and titanium dioxide 60-70%; The rosin is gum rosin, wood rosin, tall oil rosin or black rosin; most preferably, the rosin is black rosin; the unsaturated fatty acid content in the peanut oil is greater than 85%. With the addition of peanut oil, chiseled fish maw is softer, more adhesive and can be formulated more quickly.
[0049] According to the present invention, 15 parts of vaseline, 15 parts of kaolin, 30 parts of filler, 1 part of pigment and 1 part of fluorescent powder can form plasticine with fluorescent effect, and the production place of the plasticine is Tianjin. Peanut oil is the p...
Embodiment 2
[0054] 12 parts of peanut oil,
[0055] Rosin 25 parts,
[0056] Vaseline 18 parts,
[0057] Kaolin 17 parts,
[0058] 33 parts of stuffing,
[0059] 1 part paint,
[0060] Phosphor powder 1 part;
[0061] Wherein, the filler includes calcium carbonate, alumina and silicon dioxide; the fineness of the filler is 200 mesh-300 mesh; the fluorescent powder includes: talcum powder 30-40% and titanium dioxide 60-70%; The rosin is gum rosin, wood rosin, tall oil rosin or black rosin; most preferably, the rosin is black rosin; the unsaturated fatty acid content in the peanut oil is greater than 85%. With the addition of peanut oil, chiseled fish maw is softer, more adhesive and can be formulated more quickly.
[0062] According to the present invention, 18 parts of vaseline, 17 parts of kaolin, 33 parts of filler, 1 part of pigment and 1 part of fluorescent powder can form plasticine with fluorescent effect, and the production place of the plasticine is Tianjin. Peanut oil is t...
Embodiment 3
[0066] 13 parts of peanut oil,
[0067] Rosin 28 parts,
[0068] Vaseline 20 parts,
[0069] Kaolin 18 parts,
[0070] 35 parts of stuffing,
[0071] 1.5 parts of pigment,
[0072]Phosphor powder 1.2 parts;
[0073] Wherein, the filler includes calcium carbonate, alumina and silicon dioxide; the fineness of the filler is 200 mesh-300 mesh; the fluorescent powder includes: talcum powder 30-40% and titanium dioxide 60-70%; The rosin is gum rosin, wood rosin, tall oil rosin or black rosin; most preferably, the rosin is black rosin; the unsaturated fatty acid content in the peanut oil is greater than 85%. With the addition of peanut oil, chiseled fish maw is softer, more adhesive and can be formulated more quickly.
[0074] According to the present invention, 20 parts of vaseline, 18 parts of kaolin, 35 parts of filler, 1.5 parts of pigment and 1.2 parts of fluorescent powder can form plasticine with fluorescent effect, and the producing area of the plasticine is Tianjin. ...
PUM