Fluorescent lamp cover, preparation method of fluorescent lamp cover and yellow fluorescent lamp
A lampshade and fluorescent technology, which is applied in the field of fluorescent lampshades and yellow light lamps, can solve the problems of insignificant improvement of light efficiency, large consumption of rare earth fluorescent resources, and hindrance of heat dissipation, so as to improve energy utilization efficiency, increase energy utilization rate, The effect of reducing energy consumption
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0020] The preparation method of the fluorescent lampshade of an embodiment provided by the present invention comprises the following steps:
[0021] Step S110: uniformly mixing the fluorescent material and the plastic substrate to obtain a mixed material;
[0022] Step S120: Process the mixed material to obtain the fluorescent lampshade, the fluorescent lampshade has photoluminescence performance; wherein:
[0023] The fluorescent material is (denoted as fluorescent material A) or (denoted as fluorescent material B) or (denoted as fluorescent material C), the R1, R2, R3 and R4 are alkyl or aromatic groups.
[0024] In some preferred embodiments, the mass ratio of the fluorescent material to the plastic substrate is between 0.01% and 1%.
[0025] In some preferred embodiments, the transparent plastic is one of polycarbonate, polypropylene or acrylic.
[0026] In some preferred embodiments, in the step of processing the mixed material to obtain the fluorescent lampshade...
Embodiment 1
[0032] Add 0.5g of fluorescent material A to 5kg of polycarbonate plastic particles, stir and mix evenly, heat at 200 degrees for 1 hour, and obtain a fluorescent lampshade by injection molding, and then combine the fluorescent lampshade with a blue LED array to obtain the whole lamp, the entire yellow light The light effect is 122.0lm / W.
Embodiment 2
[0034] Add 20g of fluorescent material B to 5kg of polypropylene granules, stir and mix evenly, and heat at 250°C for 1 hour. The mixed material is extruded to obtain a fluorescent lampshade, and then the fluorescent lampshade is combined with a positive white LED array to obtain a whole lamp. The entire yellow light The light effect is 153.7lm / W.
PUM
| Property | Measurement | Unit |
|---|---|---|
| thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
Login to View More