Compound refining agent and waste mineral oil refining method thereof
A technology for waste mineral oil and refining agent, which is applied in the direction of refining with metal salts and only multi-stage series refining processes, etc., can solve the problems of clogging equipment, high temperature coking, affecting basic refined oil products, etc., to prevent high temperature coking. , Improve the effect of oil products
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0017] Example 1: A compound refining agent and its method for refining waste mineral oil. The formula of the compound refining agent consists of the following components in terms of mass parts: 50 parts of sodium hydroxide, 10 parts of anhydrous sodium sulfite and metasilicon 40 parts of sodium bicarbonate; during preparation, mix the above-mentioned sodium hydroxide, anhydrous sodium sulfite and sodium metasilicate in a reaction kettle and stir evenly.
[0018] The method for refining waste mineral oil with compound refining agent, its steps are as follows:
[0019] a. Mix and dilute the prepared refining agent with water at a ratio of 1:1, and then stir it evenly with a stirring rod to obtain the required solvent;
[0020] B. Mix the obtained solvent with the waste mineral oil, the ratio is: the solvent accounts for 3% of the total waste mineral oil, after mixing, stir evenly with a stirring rod, and obtain the required mixed solution after fully mixing;
[0021] c. Put th...
Embodiment 2
[0025] Embodiment 2, the preparation steps of embodiment 2 are roughly the same as embodiment 1, and its difference is that the formula of compound refining agent is calculated by the following composition in parts by mass: 45 parts of sodium hydroxide, 7 parts of anhydrous sodium sulfite and partial 35 parts of sodium silicate; wherein, the solvent accounts for 2% of the total waste mineral oil in step b, acid clay accounts for 4% of the total base crude oil in step d, and the stirring time in step e is 10 minutes; the rest are the same as in the examples 1.
Embodiment 3
[0026] Embodiment 3, the preparation procedure of embodiment 3 is roughly the same as embodiment 1, and its difference is that the formula of compound refining agent is calculated by the following composition in parts by mass: 55 parts of sodium hydroxide, 13 parts of anhydrous sodium sulfite and partial 45 parts of sodium silicate; wherein, the solvent accounts for 4% of the total waste mineral oil in step b, acid clay accounts for 6% of the total base crude oil in step d, and the stirring time in step e is 20 minutes; all the other are the same as in the examples 1.