Novel environment-friendly degradable highly-simulated bait
An artificial fish, environmental protection technology, applied in the field of fishing supplies, can solve the problems of low market share, expensive raw materials, marine organisms and ecological environment hazards, etc., and achieve low production costs, good degradability, and good mechanical properties Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
specific Embodiment 1
[0021] A new type of environmentally friendly degradable high-simulation fishing bait, including 20 parts of PPC, 10 parts of 1,4-butanediol, 30 parts of MDI, 50 parts of PLA, 30 parts of corn starch, 1 part of filler, 1 part of lubricant, and 2 parts of foaming agent , 13 parts of carbon dioxide, 10 parts of citrate plasticizer, 10 parts of amino acid, 5 parts of polylactic acid, and 6 parts of protein.
[0022] Its preparation method comprises the following steps:
[0023] Step 1: Dehydrate PPC and 1,4-butanediol at 120°C, then mix with MDI, amino acid and polylactic acid, mix the mixed raw materials into the upper hopper of the extruder, and add them in the extruder temperature, shear plasticization in the screw, the extrusion temperature is 140-220°C, the time for the material in the extruder is 15 minutes, at a temperature of 150°C-200°C and a pressure of 20-35MPa, add protein and carbon dioxide, inject In the mold, when the temperature drops to 60°C-80°C, open the mold ...
specific Embodiment 2
[0034] A new type of environmentally friendly degradable high-simulation fishing bait, including 30 parts of PPC, 15 parts of 1,4-butanediol, 40 parts of MDI, 60 parts of PLA, 40 parts of corn starch, 3 parts of filler, 5 parts of lubricant, and 4 parts of foaming agent , 15 parts of carbon dioxide, 13 parts of citrate plasticizer, 13 parts of amino acid, 9 parts of polylactic acid, and 8 parts of protein.
[0035] Its preparation method comprises the following steps:
[0036] Step 1: Dehydrate PPC and 1,4-butanediol at 120°C, then mix with MDI, amino acid and polylactic acid, mix the mixed raw materials into the upper hopper of the extruder, and add them in the extruder temperature, shear plasticization in the screw, the extrusion temperature is 140-220°C, the time for the material in the extruder is 15 minutes, at a temperature of 150°C-200°C and a pressure of 20-35MPa, add protein and carbon dioxide, inject In the mold, when the temperature drops to 60°C-80°C, open the mol...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com