Self-cleaning type tempered glass and manufacturing method thereof
A tempered glass and manufacturing method technology, applied in glass manufacturing equipment, manufacturing tools, glass molding, etc., can solve problems such as high thermal cracking tendency, reduced adhesion, poor impact resistance, etc., and achieve rapid water droplet formation and water absorption Fast speed, fast aging effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0029] A kind of self-cleaning tempered glass, its essential body composition includes silicon dioxide 85Kg, sodium oxide 15Kg by weight; The outer surface of the cured film is also integrated with a layer of finely packed silica powder with a diameter of 5 μm-8 μm.
[0030] The above-mentioned manufacturing method of self-cleaning tempered glass comprises the following steps:
[0031] 1) Preparation before production
[0032] ① Preparation of glass raw materials: prepare 85Kg of silicon dioxide and 15Kg of sodium oxide by weight;
[0033] ② Preparation of surface modification materials: sufficient amount of polyethylene film, 10Kg of corn starch, sufficient amount of acrylic acid, sufficient amount of sodium hydroxide, sufficient amount of silica powder with a diameter of 5μm-8μm, and sufficient amount of N-N'methylene-bisacrylamide crosslinking agent;
[0034] 2) Firing of the glass body
[0035] ① Mix the silicon dioxide and sodium oxide prepared in step ① in 1) evenly ...
Embodiment 2
[0052] A kind of self-cleaning tempered glass, its essential body composition includes silicon dioxide 90Kg, sodium oxide 10Kg by weight; The outer surface of the cured film is also integrated with a layer of finely packed silica powder with a diameter of 5 μm-8 μm.
[0053] The above-mentioned manufacturing method of self-cleaning tempered glass comprises the following steps:
[0054] 1) Preparation before production
[0055] ① Preparation of glass raw materials: prepare 90Kg of silicon dioxide and 10Kg of sodium oxide by weight;
[0056] ② Preparation of surface modification materials: sufficient amount of polyethylene film, 8Kg of corn starch, sufficient amount of acrylic acid, sufficient amount of sodium hydroxide, sufficient amount of silica powder with a diameter of 5μm-8μm, and sufficient amount of N-N'methylene-bisacrylamide crosslinking agent;
[0057] 2) Firing of the glass body
[0058] ① Mix the silicon dioxide and sodium oxide prepared in step ① in 1) evenly t...
PUM
| Property | Measurement | Unit |
|---|---|---|
| diameter | aaaaa | aaaaa |
| transmittivity | aaaaa | aaaaa |
| transmittivity | aaaaa | aaaaa |