Regulating method for zinc oxide flotation froth
A zinc oxide and foam technology, applied in the field of foam control in zinc oxide sorting and zinc oxide flotation foam regulation, can solve the problems of difficulty in controlling the amount of foam, poor foam structure, poor flotation index, etc., and increase the surface area. , Improve the foam structure, the effect of being conducive to recycling
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0014] The example of the regulation and control method of zinc oxide flotation foam of the present invention is made up of the following steps:
[0015] (1) Prepare combined defoamer: mix tributyl phosphate by weight: lauryl mercaptan: kerosene = 20:5:1, dissolve in water, and make a solution with a weight concentration of 20%,
[0016] (2) The solution prepared in (1) was stirred for 30 minutes until a uniform and stable pale yellow liquid was formed,
[0017] (3) When adding the prepared combined defoamer to adjust the foam during the flotation process, in order to facilitate the observation of the change in the height of the foam layer and the change in the foam structure, the baffle plate is used to raise the partition plate in the flotation cell of the flotation machine to the same level as A columnar space is formed at the same height on both sides of the tank to control the foam. After adding various chemicals in this columnar space, inflate with a fixed amount of air,...
example
[0019] The second example of the regulation and control method of zinc oxide flotation foam of the present invention is made up of the following steps:
[0020] (1) Prepare combined defoamer: mix tributyl phosphate by weight: dodecyl mercaptan: kerosene=16:4:1.5, dissolve in water, and make a solution with a weight concentration of 20%,
[0021] Steps (2 and (3) are the same as in Example 1.
Embodiment 3
[0023] The third example of the regulation and control method of zinc oxide flotation foam of the present invention is made up of following steps:
[0024] (1) Prepare combined defoamer: mix tributyl phosphate by weight: lauryl mercaptan: kerosene=30:2:1, dissolve in water, and make a solution with a weight concentration of 20%,
[0025] Steps (2 and (3) are the same as in Example 1.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com