[0017] Component A: 15 kg of ethyl acetate, 15 kg of n-butyl acetate, 5 kg of cyclohexanone, 1 kg of polyketone resin, 5 kg of 1 / 16 second nitrocellulose, 2 kg of high-efficiency matting powder, 45 kg of hydroxyl polyacrylic resin 1 kg of matt wax paste, 0.1 kg of polyether modified polydimethylsiloxane;
[0018] Component B: 25 kg of ethyl acetate, 20 kg of n-butyl acetate, 5 kg of 1,6-hexamethylene diisocyanate, 45 kg of isocyanate adduct, and 15 kg of matte trimer curing agent.
[0019] After the production of components A and B is completed, mix them with banana water in a ratio of 4:1:3, stir evenly, and then they can be used for spraying.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com