A technology of cationic rosin gum and emulsifier, which is applied in the direction of water-repellent addition, etc., can solve the problems of poor emulsion stability, high emulsification cost, out-of-control reaction, etc., and achieve the effect of preventing metal ion interference, good effect and stable quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0030] A kind of preparation method of cationic rosin latex emulsifier, comprises steps:
[0031] Feed 15kg nitrogen into the reactor, add 70kg dimethylaminoethyl methacrylate, 20kg styrene, 2kg chitosan (the weight-average molecular weight is 200,000, and the degree of deacetylation is 80%), 130kg glacial acetic acid, 450kg Mix deionized water, 5kg acrylic acid, 60kg acrylamide and 6kg potassium tartrate evenly, set the rotation speed at 170 rpm, add 3kg potassium persulfate when the temperature in the kettle reaches 50°C, and time the reaction when the temperature in the kettle reaches 80°C After 2 hours, 2 kg of potassium persulfate was added, and the reaction was continued at 80° C. for 1 hour to obtain a reaction solution. Additional water was added until the solid content reached 35 wt%, and reaction distillation was carried out at 102° C. for 1 h. Cool to room temperature, discharge, and add water until the solid content is 30 wt%, to obtain a transparent rosin latex e...
Embodiment 2
[0034] A kind of preparation method of cationic rosin latex emulsifier, comprises steps:
[0035] Pass into 24kg nitrogen in the reactor, add 60kg dimethylaminoethyl methacrylate, 25kg styrene, 2kg chitosan (the weight-average molecular weight is 150,000, and the degree of deacetylation is 90%), 120kg glacial acetic acid, 500kg Mix deionized water, 8kg acrylic acid, 70kg acrylamide and 5kg potassium tartrate evenly, set the rotation speed at 150 rpm, add 3kg potassium persulfate when the temperature in the kettle reaches 40°C, and time the reaction when the temperature in the kettle reaches 90°C After 2 hours, 3kg of potassium persulfate was added, and the reaction was continued at 90°C for 1 hour to obtain a reaction solution. Additional water was added to adjust the solid content to 30 wt%, and reaction distillation was carried out at 110° C. for 1 h. Cool to room temperature, discharge, and add water until the solid content is 25 wt%, to obtain a transparent rosin latex em...
Embodiment 3
[0038] A kind of preparation method of cationic rosin latex emulsifier, comprises steps:
[0039]Feed 15kg nitrogen into the reactor, add 65kg dimethylaminoethyl methacrylate, 23kg styrene, 2kg chitosan (weight average molecular weight is 300,000, deacetylation degree is 95%), 150kg glacial acetic acid, 200kg Mix deionized water, 6kg acrylic acid, 65kg acrylamide and 8kg potassium tartrate evenly, set the rotation speed at 190 rpm, add 1.2kg potassium persulfate when the temperature in the kettle reaches 60°C, and when the temperature in the kettle reaches 70°C, time After reacting for 2 hours, 0.8 kg of potassium persulfate was added, and the reaction was continued at 70° C. for 2 hours to obtain a reaction solution. Water was added to adjust the solid content to 40 wt%, and reaction distillation was carried out at 90° C. for 2 hours. Cool to room temperature, discharge, and add water until the solid content is 35 wt%, to obtain a transparent rosin latex emulsifier.
[0040...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com