A blank and horn technology is applied in the field of the preparation of horn comb blanks, which can solve the problems of no hand feeling, increased waste, burning, etc., and achieve the effects of improving product quality and service life, reducing waste generation, and reducing production costs.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0013] A kind of preparation method of horn comb blank, described preparation method comprises the following steps:
[0014] (1) Making the initial blank: Select horns with a shape and thickness suitable for making combs, wash and dry the selected horns naturally, and place them for 4 months, then cut off the leftovers, and then extend along the horns to the For the direction of the bull’s head, cut the bull’s horns from the middle to make a horn comb blank, and set aside;
[0015] (2) Softening treatment: Put the initial blank of the horn comb made in step (1) into heat-conducting oil at a temperature of 125°C, and perform a heating and softening treatment for 5 minutes; then put the softened horn comb blank into In the constant temperature hot pressing device, a pressure of 8 tons is used to flatten and straighten the horns. The temperature of the constant temperature hot pressing is controlled between 135 and 140°C, and the time for flattening and straightening is controlle...
Embodiment 2
[0018] A kind of preparation method of horn comb blank, described preparation method comprises the following steps:
[0019] (1) Making the initial blank: Select horns with a shape and thickness suitable for making combs, wash and dry the selected horns naturally, and place them for 5 months before cutting off the leftovers, and then stretching along the horns to the For the direction of the bull’s head, cut the bull’s horns from the middle to make a horn comb blank, and set aside;
[0020] (2) Softening treatment: Put the initial blank of the horn comb made in step (1) into the heat-conducting oil with a temperature of 128°C, and carry out a heating and softening treatment for 4 minutes; then put the initial blank of the horn comb after softening into In the constant temperature hot pressing device, 10 tons of pressure are used to flatten and straighten the horns. The temperature of the constant temperature hot pressing is controlled between 138-142°C, and the flattening and ...
Embodiment 3
[0023] A kind of preparation method of horn comb blank, described preparation method comprises the following steps:
[0024] (1) Making the initial blank: Select horns with a shape and thickness suitable for making combs, wash and dry the selected horns naturally, and place them for 6 months before cutting off the leftovers, and then stretching along the horns to the For the direction of the bull’s head, cut the bull’s horns from the middle to make a horn comb blank, and set aside;
[0025] (2) Softening treatment: Put the initial blank of the horn comb made in step (1) into the heat transfer oil with a temperature of 130°C, and carry out a heating and softening treatment for 3 minutes; then put the initial blank of the horn comb after softening into In the constant temperature hot pressing device, a pressure of 10 tons is used to flatten and straighten the horns. The temperature of the constant temperature hot pressing is controlled between 142 and 145°C, and the time for fla...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com