A cotton-polyester blending and yarn technology, applied in textiles and papermaking, plant fibers, fiber processing and other directions, can solve problems such as performance needs to be improved, and achieve the effects of improved strength, yarn hairiness, and good elongation retention performance.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0025] The sizing process of cotton-polyester blended fabric yarn comprises the following steps:
[0026] 1) Add 1 to 2 parts by weight of carbonyl diamide, 0.8 parts by weight of calcium chloride, 1.9 parts by weight of vinyl acetate resin, 1.6 parts by weight of hydroxypropyl methylcellulose, and 8 parts by weight of modified starch into 20 parts by weight in sequence In deionized water, stir evenly;
[0027] 2) Add 1.6 parts by weight of lauryltrimethylammonium chloride, 1.1 parts by weight of fatty alcohol polyoxyethylene ether, 0.9 parts by weight of sodium dodecylbenzenesulfonate, and 1.1 parts by weight of alkylsulfonate in turn, and continue stirring , until fully mixed evenly to obtain a slurry;
[0028] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 2
[0030] The sizing process of cotton-polyester blended fabric yarn comprises the following steps:
[0031] 1) Put 1 part by weight of carbonyl diamide, 0.8 parts by weight of calcium chloride, 1.9 parts by weight of vinyl acetate resin, 1.6 parts by weight of hydroxypropyl methylcellulose, and 8 parts by weight of modified starch into 20 parts by weight of deionized starch in sequence water, stir well;
[0032] 2) Add 1.6 parts by weight of lauryltrimethylammonium chloride, 1.1 parts by weight of fatty alcohol polyoxyethylene ether, 0.9 parts by weight of sodium dodecylbenzenesulfonate, and 1.1 parts by weight of alkylsulfonate in turn, and continue stirring , until fully mixed evenly to obtain a slurry;
[0033] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
Embodiment 3
[0035] The sizing process of cotton-polyester blended fabric yarn comprises the following steps:
[0036] 1) Put 2 parts by weight of carbonyl diamide, 0.8 parts by weight of calcium chloride, 1.9 parts by weight of vinyl acetate resin, 1.6 parts by weight of hydroxypropyl methylcellulose, and 8 parts by weight of modified starch into 20 parts by weight of deionized starch in sequence. water, stir well;
[0037] 2) Add 1.6 parts by weight of lauryltrimethylammonium chloride, 1.1 parts by weight of fatty alcohol polyoxyethylene ether, 0.9 parts by weight of sodium dodecylbenzenesulfonate, and 1.1 parts by weight of alkylsulfonate in turn, and continue stirring , until fully mixed evenly to obtain a slurry;
[0038] 3) Immerse the yarn in the size solution for sizing, press off the remaining solution, and dry.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com