High stability palm oil leather fatliquoring agent and preparation method thereof
A leather fatliquoring agent with high stability technology, applied in leather impregnation, small raw hide/big raw hide/leather/fur treatment, small raw hide/big raw hide/leather skin/fur chemical treatment, etc., can solve high freezing point and low temperature Poor fluidity, few research reports, etc., to achieve the effect of increasing low temperature fluidity, strong ability to disperse natural oil, and good emulsifying power
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0020] Embodiment 1: a kind of high stability palm oil leather fatliquoring agent, it is made up of the raw material composition of following parts by weight: 50 parts of modified palm oils, 25 parts of beeswax liquids, 20 parts of isotridecanyl myristate , 3 parts of coconut acid diethanolamide, 3 parts of maleic modified rosin, 1.5 parts of isobutanol, and 65 parts of water.
[0021] Further, the preparation method of the modified palm oil is: palm oil, a 1:1 mixture of monoethanolamine and diethanolamine with a mass percentage of palm oil of 15%, and sodium methoxide with a mass percentage of palm oil of 1.2% are mixed at 60°C. Stir and react for 4 hours to obtain primary modified palm oil; then lower the temperature to 45°C, add phosphorus pentoxide powder with a mass percentage of 45% of primary modified palm oil, after the addition is completed, heat up to 75°C for 3 hours, and neutralize to pH 6~7 to obtain modified palm oil; the palm oil is 12 degree palm oil; the phos...
Embodiment 2
[0028] Embodiment 2: a kind of high stability palm oil leather fatliquoring agent, it is made up of the raw material composition of following parts by weight: 40 parts of modified palm oils, 20 parts of beeswax liquids, 15 parts of isotridecyl myristate , 2 parts of coconut acid diethanolamide, 2 parts of maleic modified rosin, 1 part of isobutanol, and 60 parts of water.
[0029] Further, the preparation method of the modified palm oil is as follows: palm oil, a 1:1 mixture of monoethanolamine and diethanolamine with a mass percentage of palm oil of 10%, and sodium methoxide with a mass percentage of palm oil of 1% are mixed at 60°C. Stir and react for 4 hours to obtain primary modified palm oil; then lower the temperature to 45°C, add phosphorus pentoxide powder with a mass percentage of 40% of primary modified palm oil, and heat up to 75°C for 3 hours after the addition is completed, then neutralize to pH 6~7 to obtain modified palm oil; the palm oil is palm oil of 8 degree...
Embodiment 3
[0036] Embodiment 3: a kind of high stability palm oil leather fatliquoring agent, it is made up of the raw material composition of following parts by weight: 55 parts of modified palm oils, 30 parts of beeswax liquids, 25 parts of isotridecyl myristate , 4 parts of coconut acid diethanolamide, 4 parts of maleic modified rosin, 2 parts of isobutanol, and 70 parts of water.
[0037] Further, the preparation method of the modified palm oil is as follows: palm oil, a 1:1 mixture of monoethanolamine and diethanolamine which is 20% by mass percent of palm oil, and sodium methoxide which is 1.5% by mass percent of palm oil are mixed at 60° C. Stir and react for 4 hours to obtain primary modified palm oil; then lower the temperature to 45°C, add phosphorus pentoxide powder which is 50% of the mass percentage of primary modified palm oil, after the addition is completed, heat up to 75°C for 3 hours, and neutralize to pH 6~7 to obtain modified palm oil; the palm oil is 24 degree palm o...