Embodiment 1
[0022] The present invention proposes a kind of preparation method of green environmental protection inner wall latex, comprises the following steps:
[0023] S1. Weigh water, dispersant, surfactant, film-forming aid, defoamer, thickener, and fungicide into the batching tank according to the proportion, and stir at a low speed for 5-10 minutes;
[0024] S2, then add fillers and pigments, disperse at high speed for about 30 minutes, and enter the sand mill (or other grinding equipment) to grind to a fineness below 50 μm;
[0025] S3, add the solution obtained in S2 into the paint tank, then add the emulsion, and start stirring at a low speed for 10-13 minutes;
[0026] S4, adding defoamer and preservative, here the defoamer adopts SPA-102 compound defoamer composed of ether ester compound and organic phosphate; preservatives are sodium pentachlorophenate, phenylmercury acetate and tributyltin, etc. , the efficiency of phenolic compounds is low, the dosage is generally 0.2%, th...
Embodiment 2
[0031] The present invention proposes a kind of preparation method of green environmental protection inner wall latex, comprises the following steps:
[0032] S1. Weigh water, dispersant, surfactant, film-forming aid, defoamer, thickener, and fungicide into the batching tank according to the proportion, and stir at a low speed for 5-10 minutes;
[0033] S2, then add fillers and pigments, disperse at high speed for about 30 minutes, and enter the sand mill (or other grinding equipment) to grind to a fineness below 50 μm;
[0034] S3, add the solution obtained in S2 into the paint tank, then add the emulsion, and start stirring at a low speed for 10-13 minutes;
[0035] S4, adding defoamer and preservative, here the defoamer adopts SPA-102 compound defoamer composed of ether ester compound and organic phosphate; preservatives are sodium pentachlorophenate, phenylmercury acetate and tributyltin, etc. , the efficiency of phenolic compounds is low, the dosage is generally 0.2%, th...
Embodiment 3
[0040] The present invention proposes a kind of preparation method of green environmental protection inner wall latex, comprises the following steps:
[0041] S1. Weigh water, dispersant, surfactant, film-forming aid, defoamer, thickener, and fungicide into the batching tank according to the proportion, and stir at a low speed for 5-10 minutes;
[0042] S2, then add fillers and pigments, disperse at high speed for about 30 minutes, and enter the sand mill (or other grinding equipment) to grind to a fineness below 50 μm;
[0043] S3, add the solution obtained in S2 into the paint tank, then add the emulsion, and start stirring at a low speed for 10-13 minutes;
[0044] S4, adding defoamer and preservative, here the defoamer adopts SPA-102 compound defoamer composed of ether ester compound and organic phosphate; preservatives are sodium pentachlorophenate, phenylmercury acetate and tributyltin, etc. , the efficiency of phenolic compounds is low, the dosage is generally 0.2%, th...