Ore floatation collecting agent for oxidized ore
A technology for mineral flotation and collectors, applied in flotation, solid separation and other directions, can solve the problems of unacceptable enterprises, complicated preparation methods, and high production costs, and achieve enhanced selectivity, improved collection efficiency, and increased ore loading. amount of effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] Weigh the corresponding components according to the proportion, wherein: the weight percentage proportion of dibutyl ammonium dithiophosphate is 1%, the weight percentage proportion of oxidized paraffin wax soap is 30%, the weight percentage proportion of sodium edetate Ratio is 21%, the weight percent distribution ratio of disodium maleate dihydrate is 10%, and the balance is water.
[0026] First, mix dibutyl ammonium dithiophosphate, oxidized paraffin wax soap and part of water, heat to 60-80°C and stir for 0.5-1.5h to obtain component A. Add salt and disodium maleate dihydrate to the remaining water and stir for 2-4 hours to obtain component B, add the prepared component A to component B and stir evenly to obtain the oxidized ore mineral flotation collection Agent 1.
Embodiment 2
[0028] Weigh the corresponding components according to the proportion, wherein: the weight percentage proportion of dibutyl ammonium dithiophosphate is 5%, the weight percentage proportion of oxidized paraffin wax soap is 31%, the weight percentage proportion of sodium edetate Ratio is 25%, the weight percent distribution ratio of disodium maleate dihydrate is 10%, and the balance is water.
[0029] First, mix dibutyl ammonium dithiophosphate, oxidized paraffin wax soap and part of water, heat to 60-80°C and stir for 0.5-1.5h to obtain component A, and ethylenediaminetetraacetic acid at 50-60°C Sodium and disodium maleate dihydrate are added to the remaining water and stirred for 2-4 hours to obtain component B, and the prepared component A is added to component B and stirred evenly to obtain the oxidized ore mineral flotation collector 2.
Embodiment 3
[0031] Weigh the corresponding components according to the proportion, wherein: the weight percentage proportion of dibutyl ammonium dithiophosphate is 10%, the weight percentage proportion of oxidized paraffin wax soap is 31%, the weight percentage proportion of sodium edetate Ratio is 25%, the weight percent distribution ratio of disodium maleate dihydrate is 15%, and the balance is water.
[0032] First, mix dibutyl ammonium dithiophosphate, oxidized paraffin wax soap and part of water, heat to 60-80°C and stir for 0.5-1.5h to obtain component A, and ethylenediaminetetraacetic acid at 50-60°C Sodium and disodium maleate dihydrate are added to the remaining water and stirred for 2-4 hours to obtain component B, and the prepared component A is added to component B and stirred evenly to obtain the oxidized ore mineral flotation collector 3.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com