High-strength waterborne wood coating and manufacturing method thereof

A technology of wood coatings and manufacturing methods, which is applied in the direction of antifouling/underwater coatings, coatings, paints containing biocide, etc., can solve the problems of poor bonding, poor bonding of wood, and easy wear and tear, so as to improve strength, Effect of improving wear resistance and bonding force

Inactive Publication Date: 2019-03-12
JIANGSU HIMONIA TECH
View PDF6 Cites 2 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

[0002] At present, wooden utensils are common in our lives, and their surface paints have great limitations: they are easy to age and peel off, and most of them are organic polymers with high formaldehyde content. Looking at the entire domestic wood utensils market, there are many varieties, but Most of them have the functions of protection, sealing and decoration. Most of the functional coatings are coatings with water resistance, alkali resistance, stain resistance and relatively simple flame retardancy, and most of them are organic-based coatings, which contain harmful substances. components; a small amount of water-based paint has obvious defects such as poor sealing ability or poor bonding with wood
[0004] Among the relevant patents that have been applied in China, the patent "A Waterborne Acrylic Wood Sealing Coating and Preparation Method of Its Special Emulsion" (application number: 201010159689.4, publication date: 2010.09.01) discloses an acrylic paint for wood sealing. The copolymer emulsion of the present invention has excellent sealing performance, but without the addition of reinforcing functional substances, its binding force is poor, and it is also easy to be worn and peeled; in addition, other main material components of the invention are prone to produce toxic and harmful substances at high temperatures
The patent "Water-based Wood Lacquer Emulsion" (application number: 200810081974.1, publication date: 2009.09.09) discloses a high-temperature-resistant and water-resistant emulsion, which obtains stable silicon-oxygen bonds by adding silica sol, thereby improving the high-temperature resistance of the emulsion performance, but it has high solid content and is easy to crack; at the same time, there is no additive with adhesion promotion function, and the binding force is poor

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0029]A high-strength water-based wood coating, the water-based wood coating is based on 70Kg of urethane acrylate grafted acrylate, 18Kg of starch grafted sodium acrylate, 1.5Kg of potassium hydroxide, 0.3Kg of aluminum borate whiskers, and 2Kg of silicon carbide powder in parts by weight. , CF carbon fiber 8Kg, tackifier extracted from goat horn 35Kg, blocked isocyanate 3Kg, polyether-siloxane copolymer 0.3Kg, water-based adhesion promoter extracted from peach branch 10Kg as raw materials, deionized Water is the medium, and it is fully reacted at 80°C-85°C; the preparation process of the tackifier includes soaking, dicing, stewing, purification, and concentration; the preparation process of the water-based adhesion promoter includes foaming, microbial wall breaking, Collagen is released, activated and concentrated.

[0030] A kind of manufacture method of high-strength waterborne wood coating, comprises the following steps:

[0031] 1) Raw material preparation

[0032] ① P...

Embodiment 2

[0048] The whole is consistent with Example 1, the difference is:

[0049] A kind of high-strength water-based woodware coating, this water-based woodware coating is by weight polyurethane acrylate graft acrylate 80Kg, starch grafted sodium acrylate 15Kg, ammonium hydroxide 1Kg, aluminum borate whisker 0.2Kg, silicon carbide powder 1Kg, CF carbon fiber 5Kg, tackifier extracted from goat horn 30Kg, blocked isocyanate 2Kg, polyether-siloxane copolymer 0.2Kg, water-based adhesion promoter extracted from peach branch 8Kg as raw materials, deionized water As the medium, it is fully reacted at 70°C-75°C; the preparation process of the tackifier includes infiltration, dicing, stewing, purification, and concentration; the preparation process of the water-based adhesion promoter includes foaming, microbial wall breaking, and collagen Substance release and activation, concentration.

[0050] A kind of manufacture method of high-strength waterborne wood coating, comprises the following ...

Embodiment 3

[0064] The whole is consistent with Example 1, the difference is:

[0065] A high-strength water-based wood coating, the water-based wood coating is based on 75Kg of urethane acrylate grafted acrylate, 16Kg of starch grafted sodium acrylate, 0.6Kg of sodium hydroxide, 0.5Kg of ammonium hydroxide, and 0.25 kg of aluminum borate whiskers in parts by weight. Kg, silicon carbide powder 1.5Kg, CF carbon fiber 6Kg, tackifier extracted from goat horn 32Kg, blocked isocyanate 2.5g, polyether-siloxane copolymer 0.25Kg, water-based adhesion extracted from peach branch 9Kg Accelerator as raw material, deionized water as medium, fully reacted at 75°C-80°C; the preparation process of the tackifier includes infiltration, dicing, stewing, purification, and concentration; the preparation process of the water-based adhesion promoter Including hair foaming, microbial wall breaking, collagen release and activation, and concentration.

[0066] A kind of manufacture method of high-strength waterb...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

PropertyMeasurementUnit
particle diameteraaaaaaaaaa
Login to view more

Abstract

The invention discloses a high-strength waterborne wood coating and a manufacturing method thereof. The high-strength waterborne wood coating is prepared by taking polyurethane acrylate grafted acrylate, starch grafted sodium acrylate, water-soluble alkali, aluminum borate whisker, silicon carbide powder, CF (carbon fiber), tackifier extracted from cornu gorais powder, blocked isocyanate, polyether-siloxane copolymer, and aqueous adhesion promoter as raw materials and deionized water as medium for sufficient reaction at 70-85 DEG C, wherein the tackifier is prepared through the steps of moisturizing, pelletizing, boiling, purifying and concentrating; the waterborne adhesion promoter is prepared through the steps of soaking, microorganism fragmentation, collagen releasing and activating, and concentrating. The high-strength waterborne wood coating has the technical advantages of being applicable to wood surface, waterborne, free from damage to wood, high in strength and wearing resistance, lubricant in surface and good in texture.

Description

technical field [0001] The invention relates to the field of wood coatings, in particular to a high-strength water-based wood coating and a manufacturing method thereof. Background technique [0002] At present, wooden utensils are common in our lives, and their surface paints have great limitations: they are easy to age and peel off, and most of them are organic polymers with high formaldehyde content. Looking at the entire domestic wood utensils market, there are many varieties, but Most of them have the functions of protection, sealing and decoration. Most of the functional coatings are coatings with water resistance, alkali resistance, stain resistance and relatively simple flame retardancy, and most of them are organic-based coatings, which contain harmful substances. components; a small amount of water-based paint has obvious defects such as poor sealing ability or poor bonding with wood. [0003] At present, in the conventional technology in this field, persulfate or...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C09D151/08C09D151/02C09D7/61C09D7/63C09D7/65C09D5/14
CPCC08L2205/02C08L2205/035C09D5/14C09D7/61C09D7/63C09D7/65C09D7/70C09D151/08C08L51/02C08L93/00C08K13/04C08K7/06C08K7/08
Inventor 吴志飞陈明贵常红言
Owner JIANGSU HIMONIA TECH
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products