Preparation method of watertight cable filling sealant and application of watertight cable filling sealant in cable products
A watertight cable and sealant technology, which is applied in cable/conductor manufacturing, circuits, adhesives, etc., can solve the problems of viscosity, high and low temperature resistance, and poor effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] Embodiment 1: A method for preparing a watertight cable filling sealant, comprising the following steps:
[0025] 1) First, use natural SiO2 high-precision grinding technology to prepare nano-SiO2 powder;
[0026] 2) TDI modified nano-SiO2: add an appropriate amount of nano-SiO2 to the reaction device protected by N2, dilute with 3,5-dimethylthiotoluenediamine and stir, stir at 100 rpm for ten minutes, ultrasonic Disperse for 15 minutes, add an appropriate amount of TDI (2,4 toluene diisocyanate), ultrasonically disperse for ten minutes, heat with mechanical stirring, keep the reaction temperature at about 80°C, keep the reaction temperature, after reacting for 2 hours, then add an appropriate amount of polyether ( Polyoxypropylene diol), after maintaining the temperature and continuing to react for 1 hour, the TDI modified nano-SiO2 powder was prepared;
[0027] 3) Preparation of the first adhesive matrix: Pre-polymerization reaction is used to dry polyether (polyoxyp...
PUM
Property | Measurement | Unit |
---|---|---|
Glass transition temperature | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap