One-step-method production process of ultra-fine nylon and polyester blended filament yarn
A production process and technology of mixed filament yarn, applied in the field of one-step production process of ultra-fine nylon polyester mixed filament yarn, to achieve the effect of short process flow and stable product quality
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0025] to combine Figure 1 to Figure 2 , to describe this embodiment in detail. The one-step production process of ultra-fine nylon and polyester blended filaments involved in this embodiment includes the following steps: S1 slice drying, S2 spinning of nylon 6 part, S3 spinning of polyester POY part, S4 nylon 6 and polyester POY Grid tie and S5 winding.
[0026] Drying of slices in step S1: hot air drying of nylon 6 slices and PET slices in a hot air drying device, so that the moisture content of nylon 6 slices is ≦19×10 -6 , fluctuation value≦5×10 -6 ;The moisture content of PET chips≦25×10 -6 , fluctuation value≦5×10 -6 .
[0027] The level and uniformity of the moisture content of the chips are very important for the production of ultrafine denier fibers. The low and uniform water content can greatly reduce the thermal cracking and oxidative cracking of chips during melting, ensuring smooth production. In actual production, nylon 6 slices should ensure that the moi...
Embodiment 2
[0047] to combine Figure 1 to Figure 2 , to describe this embodiment in detail. The one-step production process of ultra-fine nylon and polyester blended filaments involved in this embodiment includes the following steps: S1 slice drying, S2 spinning of nylon 6 part, S3 spinning of polyester POY part, S4 nylon 6 and polyester POY Grid tie and S5 winding.
[0048] Drying of slices in step S1: hot air drying of nylon 6 slices and PET slices in a hot air drying device, so that the moisture content of nylon 6 slices is ≦19×10 -6 , fluctuation value≦5×10 -6 ;The moisture content of PET chips≦25×10 -6 , fluctuation value≦5×10 -6 .
[0049] The level and uniformity of the moisture content of the chips are very important for the production of ultrafine denier fibers. The low and uniform water content can greatly reduce the thermal cracking and oxidative cracking of chips during melting, ensuring smooth production. In actual production, nylon 6 slices should ensure that the moi...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com