Gas valve film, preparation method thereof and laminating process
A gas valve film and process technology, applied in the field of gas valve film and its preparation, can solve the problems of poor impact resistance, film wrinkling, poor production and processing performance, etc., and achieve improved strength and heat resistance, good transparency and durability The effect of heat and high strength processability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0032] An air valve film, which is co-extruded and hot-pressed by sequentially stacking an outer layer, a middle layer, and an inner layer; the thickness ratio of the outer layer, the middle layer, and the inner layer is: 1:3:3, and the total The thickness is 37.5 μm; the outer layer is the first metallocene linear low density polyethylene; the middle layer is the second metallocene linear low density polyethylene; the inner layer includes the following components calculated by weight percentage: the first Metallocene linear low density polyethylene 10%, second metallocene linear low density polyethylene 85%, polyolefin elastomer 5%.
[0033] Wherein, the density of the first metallocene linear low density polyethylene is 0.915g / cm 3 , the melt index MI is 1g / 10min; the density of the second metallocene linear low density polyethylene is 0.922g / cm 3 , the melt index MI is 1g / 10min; the density of the polyolefin elastomer is 0.900g / cm 3 , Melt index MI is 1g / 10min.
[0034] ...
Embodiment 2
[0039] An air valve film, which is co-extruded and hot-pressed from an outer layer, a middle layer, and an inner layer stacked in sequence; the thickness ratio of the outer layer, the middle layer, and the inner layer is: 2:5:2, and the total The thickness is 37.5 μm; the outer layer includes the following components calculated by weight percentage: 50% of the first metallocene linear low-density polyethylene, 48% of the second metallocene linear low-density polyethylene, and 2% of open smooth masterbatch ; The middle layer includes the following components calculated by weight percentage: the first metallocene linear low density polyethylene 98%, and the opening smooth masterbatch 2%; the inner layer includes the following components calculated by weight percentage: the first 40% metallocene linear low density polyethylene, 30% second metallocene linear low density polyethylene, 30% polyolefin elastomer.
[0040] Wherein, the density of the first metallocene linear low densit...
Embodiment 3
[0046] An air valve film, which is made by co-extruding and hot-pressing an outer layer, a middle layer, and an inner layer stacked in sequence; the thickness ratio of the outer layer, the middle layer, and the inner layer is: 3:7:3, and the total The thickness is 37.5 μm; the outer layer includes the following components calculated by weight percentage: 86% of the first metallocene linear low-density polyethylene, 10% of the second metallocene linear low-density polyethylene, and 4% of open smooth masterbatch ; The middle layer includes the following components calculated by weight percentage: the first metallocene linear low density polyethylene 10%, the second metallocene linear low density polyethylene 86%, open smooth masterbatch 4%; the inner layer It includes the following components calculated by weight percentage: 25% of the first metallocene linear low-density polyethylene, 25% of the second metallocene linear low-density polyethylene, and 50% of polyolefin elastomer....
PUM
| Property | Measurement | Unit |
|---|---|---|
| density | aaaaa | aaaaa |
| melt flow index | aaaaa | aaaaa |
| density | aaaaa | aaaaa |
Abstract
Description
Claims