Multifunctional health-care purple sand filtering water-purifying material and manufacturing method thereof
A multi-functional, purple sand technology, applied in the field of water purification, can solve the problem that the functionality cannot well meet the requirements of healthy drinking water, and achieve the effect of uniform pore size distribution
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0034] 1, a kind of purple sand filter water purification material with multifunctional health care of the present embodiment, its raw material is composed of: purple sand ore 46wt%, composite mineral calcined grain (average particle size 40 orders, particle size range 20~60 orders) 24wt%, bamboo charcoal (average particle size 60 mesh, particle size range 30-100 mesh) 9wt%, coconut shell powder (average particle size 50 mesh, particle size range 40-60 mesh) 13wt%, Chinese fir chips (average particle size 30 mesh, particle size range 20-40 mesh) 4wt%, calcite 2.3wt%, sodium humate 1.5wt%, CMC 0.2wt%.
[0035] Among them, the raw material composition of the composite mineral calcined grains is: 35wt% of medical stone, 33wt% of muyu stone, 12wt% of selenium-enriched rock powder, 10wt% of tourmaline, and 10wt% of monazite.
[0036] 2, the above-mentioned manufacturing method of the purple sand filter water purification material with multifunctional health care of the present embo...
Embodiment 2
[0044] This embodiment has a multifunctional health care purple sand filter water purification material and its manufacturing method, which differs from Embodiment 1 in that:
[0045] 1. In this embodiment, a kind of purple sand filter water purification material with multifunctional health care is composed of raw materials: 44wt% of purple sand ore, 23wt% of composite mineral calcined grains, 10wt% of bamboo charcoal, 15wt% of coconut shell powder, and 4wt% of fir chips , Calcite 2.5wt%, sodium humate 1.3wt%, CMC 0.2wt%.
[0046] Among them, the raw material composition of the composite mineral calcined grain is: 36wt% of medical stone, 35wt% of muyu stone, 10wt% of selenium-enriched rock powder, 12wt% of tourmaline, and 7wt% of monazite.
[0047] 2. In the manufacturing method step (1) of the preparation of the composite mineral calcined grains, the calcining temperature is 1050° C. and the holding time is 25 minutes; in step (2-3), the calcining temperature is 1080° C. and ...
Embodiment 3
[0049] This embodiment has a multifunctional health care purple sand filter water purification material and its manufacturing method, which differs from Embodiment 1 in that:
[0050] 1. In this embodiment, a purple sand filter and water purification material with multifunctional health care is composed of raw materials: 48wt% of purple sand ore, 25wt% of calcined composite mineral grains, 8wt% of bamboo charcoal, 12wt% of coconut shell powder, and 2.5wt% of fir chips %, calcite 3wt%, sodium humate 1.3wt%, CMC 0.2wt%.
[0051] Among them, the raw material composition of the composite mineral calcined grain is: 35wt% of medical stone, 30wt% of muyu stone, 15wt% of selenium-enriched rock powder, 12wt% of tourmaline, and 8wt% of monazite.
[0052] 2. The calcination temperature in step (2-3) of the manufacturing method of this embodiment is 1120°C.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com