A softening agent and solvent technology, which is applied in the field of high-safety non-yellowing slippery elastic softening agent and its preparation, can solve the problems of easy yellowing of products, improve hand feeling and hydrophilicity, improve emulsification effect, Good antibacterial and hand feeling effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0049] A soft finishing agent comprising a component of a component: 15 parts of amino silicone oil (ammonia value of 0.4), 8 parts of polyvinyl alcohol, 1 hydroxymethylcellulose, 1 nano-oxide, EL-20 5 parts, One acetic acid, 1 aloe extract, 3 parts of anhydrous ethanol, 10 water.
[0050] The preparation method of aloe extract includes the following steps: dry aloe vera dry, pulverize, add 5 times of 75% ethanol, ultrasonic extraction 1H, ultrasonic power 100W, filtration, filtrate, ethyl acetate, petroleum ether, extract, petroleum ether The extract was concentrated, dried.
[0051] The preparation method of the soft finishing agent includes the steps of:
[0052] (1) Mix the amino silicone oil, 50% EL-20, acetic acid, nano titanium oxide, and anhydrous ethanol, at 35 ° C ultrasonic chromogenic acid, and solution 1;
[0053] (2) Polyvinyl alcohol, hydroxymethylcellulose, and residual emulsifier, the microwave assisted dissolution, the temperature of the microwave is 20 ° C, the ...
Embodiment 2
[0056] A soft finishing agent comprising a component of the following weight: 15 parts of amino silicone oil (ammonia value of 0.4), 8 parts of polyvinyl alcohol, 1 hydroxymethylcellulose, 1 antibacterial agent, 5 emulsifiers, 1 acetic acid 1 1 part, aloe extraction, 3 parts of anhydrous ethanol, 10 water.
[0057] The antibacterial agent is nano silver, nano-oxide, zinc oxide mixtures, and the three mass ratios 1: 4: 1;
[0058] The emulsifier is EL-20, EL-40, PEG-200 and PEG-400 four compound mixed emulsifiers, four mass ratios 1: 1: 2: 3.
[0059] The preparation method of aloe extract includes the following steps: dry aloe vera dry, pulverize, add 5 times of 75% ethanol, ultrasonic extraction 1H, ultrasonic power 100W, filtration, filtrate, ethyl acetate, petroleum ether, extract, petroleum ether The extract was concentrated, dried.
[0060] The preparation method of the soft finishing agent includes the steps of:
[0061] (1) Mix the amino silicone oil, 50% emulsifier, acetic...
Embodiment 3
[0065] A soft finishing agent comprising a component of a weight component: a triple copolymer silicone oil (tetramethylene dihydroosiloxane, amino polyether compound, copolymer of allyl epoxyethylene ether), poly 12 parts of vinyl alcohol, 2 hydroxymethylcellulose, 3 antibacterial agents, 10 emulsifiers, 2 citric acid, 2 aloe vera extracts, 8 parts of isopropyl alcohol, 15 parts of water.
[0066] The antibacterial agent is a mixture of nano silver, nano-oxide, zinc oxide, and the three mass ratio 3: 8: 1;
[0067] The emulsifier is EL-20, EL-40, PEG-200 and PEG-400 four compound mixed emulsifiers, and the quadratic ratio is 1: 3: 4: 6.
[0068] The preparation method of aloe extract includes the steps: drying aloe, pulverizing aloe, adding 8 times 95% ethanol, ultrasonic extraction 2H, ultrasonic power 300W, filtration, filtrate, ethyl acetate, petroleum ether, extract, petroleum ether The extract was concentrated, dried.
[0069] The preparation method of the soft finishing age...