Concrete road paving method using soil stabilizer
A soil curing agent, a technology for concrete roads, used in chemical instruments and methods, roads, roads, etc., can solve the problems of poor resistance and easy damage of clay roadbeds, reduce moisture content, enhance stability, and reduce water. attached effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] The present invention uses the concrete road laying method of soil curing agent, comprises the following steps:
[0036] S1. Excavate the roadbed, collect soil samples of the roadbed, and measure the mineral composition and physical and chemical properties of the soil;
[0037] S2. Prepare a suitable soil curing agent according to the mineral composition and physical and chemical properties of the soil obtained in step S1;
[0038] S3, uniformly mixing the soil curing agent with the soil produced after excavating the roadbed to obtain a base soil, laying the base soil evenly on the roadbed to form a base soil layer, and forming a consolidated board after the base soil layer is solidified;
[0039] S4. After leveling the base soil layer, evenly lay cement concrete on the surface of the base soil layer, set up a fine milling layer, spray emulsified asphalt waterproof bonding layer, place steel mesh, lay sand and gravel cushion, and lay asphalt surface layer.
[0040] The...
Embodiment 2
[0055] Based on above-mentioned embodiment, the configuration method of soil solidifying agent described in step S2, comprises the following steps:
[0056] A. Obtain the base material of the soil curing agent, the base material includes a water-reducing and reinforcing powder and a liquid, and the water-reducing and reinforcing powder comprises the following components by mass fraction: 34.56% CaO, 52.1% SO 3 , 0.048% Na 2 O, 0.077% MgO, 1.7% Al 2 o 3 , 4.02% SiO 2 , 1.59%P 2 o 5 , 0.155%K 2 O, 0.145%TiO 2 , 0.0037% V 2 o 5 , 0.0043% Cr 2 o 3 , 0.875% Fe 2 o 3 , 0.0012% MnO, 0.00082% Co 3 o 4 , 0.0028% NiO, 0.39% SrO, 0.004% CuO, 0.0059% ZnO, 0.0089% Y 2 o 3 , 0.0099% ZrO 2 , 0.0042% MoO 3 , 0.0021% PdO, 0.0017% CdO, 0.0048% gold, 0.004% iodide, 0.36% fluoride, 0.013% BaO, 0.001% PtO 2 , 0.0027% HgO, 0.0027% PbO, 0.002% PuO 2 , 0.0007% Ho 2 o 3 , 0.0014% Er 2 o 3 ; The liquid preparation includes the following components by mass fraction: 20% sodium / ca...
Embodiment 3
[0061] Based on the foregoing embodiments, the cement concrete described in step S4 includes the following components in parts by weight: 300-450 parts of cement, 150-200 parts of water, 400-600 parts of sand, 20-40 parts of mineral admixture, 30- 60 parts of silicon powder, 5-10 parts of toughening agent, 1-3 parts of steel fiber.
[0062] The invention optimizes the proportion of cement concrete, so that the strength, density, viscosity and water loss of cement concrete can reach the best construction range.
PUM