Micro-emulsified mint essence for cigarette paper as well as preparation method and application of micro-emulsified mint essence
A technology of mint essence and microemulsion method, which is applied in the fields of essential oils/flavors, papermaking, paper coating, etc., can solve the problems of inability to obtain mint flavor, lack of natural flavor of mint grass, and change of aroma, and improve the smoking quality of cigarettes , The natural characteristic aroma and cool feeling of good mint, and the effect of reducing volatility
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] Weigh 15 parts of peppermint oil, 2 parts of Asian peppermint oil and 1 part by weight of menthol in parts by weight, add 18 parts of Tween 80 and 6 parts of Span 80, stir and dissolve evenly, and prepare peppermint oil-emulsifier oil Mutually;
[0024] Weigh 15 parts of α-cyclodextrin and 25 parts of distilled water in parts by weight, heat and stir in a water bath at 40°C to prepare the aqueous phase of α-cyclodextrin solution;
[0025] Add the oil phase into the water phase and stir evenly to obtain the microemulsified mint essence.
Embodiment 2
[0027] Weigh 4 parts of peppermint oil, 6 parts of Asian peppermint oil and 5 parts of menthol in parts by weight, add 10 parts of Tween 80 and 1 part of Span 80, stir and dissolve evenly, and prepare peppermint oil-emulsifier oil Mutually;
[0028] Weigh 5 parts of β-cyclodextrin and 50 parts of distilled water in parts by weight, heat and stir in a water bath at 65°C to prepare the aqueous phase of the β-cyclodextrin solution;
[0029] Add the oil phase into the water phase and stir evenly to obtain the microemulsified mint essence.
Embodiment 3
[0031] Weigh 10 parts of peppermint oil, 10 parts of Asian peppermint oil and 3 parts by weight of menthol in parts by weight, add 25 parts of Tween 80 and 5 parts of Span 80, stir and dissolve evenly, and prepare peppermint oil-emulsifier oil Mutually;
[0032] Weigh 10 parts of γ-cyclodextrin and 35 parts of distilled water in parts by weight, heat and stir in a water bath at 50°C to prepare the aqueous phase of the γ-cyclodextrin solution;
[0033] Add the oil phase into the water phase and stir evenly to obtain the microemulsified mint essence.
PUM
Property | Measurement | Unit |
---|---|---|
wavelength | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com