High-diffuse-reflection brightness enhancement coating for inner wall of greenhouse
A high diffuse reflection and greenhouse inner wall technology, applied in the field of greenhouse light enhancement, can solve problems affecting crop growth, development, yield, quality, etc., and achieve the effect of favorable quality, excellent refractive index, and excellent light scattering ability
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] Embodiment 1, a kind of greenhouse inner wall high diffuse reflection light-enhancing coating of the present invention, comprises following raw material: titanium dioxide, zirconium dioxide, paint and paint thinner, the weight ratio of described titanium dioxide, zirconium dioxide, paint and paint thinner For 77:23:400:30. The paint is a varnish.
[0016] A method for preparing a high-diffuse-reflection gloss-enhancing coating on an inner wall of a greenhouse, comprising the following steps:
[0017] Step 1: Prepare titanium dioxide, zirconium dioxide, paint and thinner in corresponding weight ratios according to parts by weight;
[0018] Step 2: Sinter titanium dioxide and zirconium dioxide in a corresponding weight ratio in a boiler at 1300°C for 2 hours, cool to room temperature, and use a ball mill to grind titanium dioxide and zirconium dioxide to mixed particles with a particle size of 8 μm;
[0019] Step 3: Prepare a clean container, put the mixed particles obt...
Embodiment 2
[0021] Embodiment 2, a kind of high diffuse reflection light-enhancing coating on the inner wall of a greenhouse of the present invention comprises the following raw materials: titanium dioxide, zirconium dioxide, paint and paint thinner, and the weight ratio of said titanium dioxide, zirconium dioxide, paint and paint thinner For 67:13:350:20. The paint is a varnish.
[0022] A method for preparing a high-diffuse-reflection gloss-enhancing coating on an inner wall of a greenhouse, comprising the following steps:
[0023] Step 1: Prepare titanium dioxide, zirconium dioxide, paint and thinner in corresponding weight ratios according to parts by weight;
[0024] Step 2: Sinter titanium dioxide and zirconium dioxide in a corresponding weight ratio in a boiler at 1300°C for 2 hours, cool to room temperature, and use a ball mill to grind titanium dioxide and zirconium dioxide to mixed particles with a particle size of 8 μm;
[0025] Step 3: Prepare a clean container, put the mixe...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com