Embodiment 1
[0010] Example 1 Take a gray cloth, add it to 10% sulfuric acid solution, degrease and wash it for 30 minutes, then bleach it with uranium bisulfite solution, soften it with vinegar-based quaternary feeding solution, and then perform preliminary presetting , unfold the fabric, and steam dry the unfolded fabric for 50 minutes.
[0011] The dried cloth adopts the method of computer printing and typesetting, three basic pigments of purple, yellow and red are used as the background color, and the chrysanthemum and willow leaf pattern of purple, orange and green are used as the basic colors. On the fabric, the thickness of the semi-finished fabric obtained is 18 times that of the finished fabric. The semi-finished fabric is dried with steam, and then it is treated in an oxygen cloud pot at 128 ℃ for 45 minutes at high temperature and high pressure to soften the pigment; then a catalyst is used to penetrate the pigment into the Creates a stable print in the fabric. Finally, the obt...
Embodiment 2
[0014] Take a piece of gray cloth, add it to 10% sulfuric acid solution for degreasing and cleaning for 35 minutes, then bleach it with uranium sulfite solution, soften it with vinegar-based quaternary solution, and then perform preliminary pre-setting, unfold the cloth , and steam dry the unfolded fabric for 25 minutes.
[0015] The dried cloth adopts the method of computer printing and typesetting, using four basic pigments of red, yellow, blue and green plus silk-screen paint as the background color, and silk-screening the lotus pattern using purple, orange and red as the basic colors on the cloth Above, the thickness of the semi-finished fabric obtained is 13 times that of the finished fabric. The semi-finished fabric is dried with steam, and then it is treated in an oxygen cloud pot at 128°C for 40 minutes at high temperature and high pressure to soften the pigment; and then a catalyst is used to infiltrate the pigment into the fabric form a stable print. Finally, the ob...
Embodiment 3
[0018] Take a piece of greige, add it to 0.8mg / ml sodium dodecyl sulfate solution for degreasing and cleaning for 45 minutes, then bleach it with sodium thiosulfate solution, soften it with fatty acid ester solution, and then make a preliminary reservation shape, unfold the fabric, and steam dry the unfolded fabric for 40 minutes.
[0019] Use the method of computer printing and typesetting on the dried cloth, use five basic pigments of black, purple, yellow, green, and red and silk screen paint as the background color, and use purple, orange, and blue as the basic color of the chrysanthemum pattern for silk screen printing On the fabric, the thickness of the semi-finished fabric obtained is 15 times that of the finished fabric. The semi-finished fabric is dried with steam, and then it is treated in an oxygen cloud pot at 128 ℃ for 55 minutes at high temperature and high pressure to soften the pigment; then use it as a catalyst to make the pigment Penetrates into the fabric to...