Breast patch and preparation method thereof
A technology of a breast patch and an adhesive layer, which is applied in the field of breast patch and its preparation, can solve the problems of affecting women's breast health, poor adhesion of the breast patch, poor support performance, etc., and achieves hard detachment, strong adhesion, and wearing comfort. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0035] Embodiment one: a kind of breast paste, comprises main adhesive layer and viscous adhesive layer, and described main adhesive layer comprises the component of following parts by weight:
[0036] 60 parts raw rubber;
[0037] 30 parts of white carbon black;
[0038] 10 parts of silicone oil. .
[0039] Specifically, an isolation layer is provided between the main adhesive layer and the adhesive adhesive layer.
[0040] Specifically, the adhesive adhesive layer is a pressure-sensitive adhesive layer.
[0041] Specifically, the main rubber layer is also added with vulcanizing agent and color glue.
[0042] Specifically, the vulcanizing agent is a low-temperature vulcanizing agent or a high-temperature vulcanizing agent.
[0043] Specifically, there are two nipple stickers 1 , and the two nipple stickers 1 are connected by buckles 2 .
[0044] see figure 1 Specifically, the buckle 2 is Z-shaped, and the two ends of the buckle 2 are respectively provided with hooks be...
Embodiment 2
[0047] Embodiment 2: A preparation method of milk paste, respectively weigh raw rubber, white carbon black and silicone oil according to the milk paste described in embodiment 1;
[0048] S1. First mix raw rubber, white carbon black and silicone oil, add vulcanizing agent and color glue and stir in the rubber mixer;
[0049] S2, cutting after forming the rubber;
[0050] S3, then put the rubber on the molding machine and form it through a mold;
[0051] S4. Remove the burr from the nipple after stamping;
[0052] S5, apply an isolation layer on the nipple 1;
[0053] S6. Brush the isolation layer and dry it for 30 minutes, then apply pressure-sensitive adhesive, and bake at 120°C for 20 minutes after brushing to complete.
[0054] Specifically, step S6 can also be replaced by:
[0055] After brushing the pressure-sensitive adhesive, let it dry naturally for 6-10 hours to complete.
PUM

Abstract
Description
Claims
Application Information

- R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com