Environment-friendly colored pavement binder and preparation method thereof
A binder and environment-friendly technology, which is applied in the field of environment-friendly colored pavement binder and its preparation, can solve the problems of endangering the health of the masses, uneven binder materials, serious light colors, etc., and achieve shortened preparation time and good compatibility sex, full color effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
preparation example Construction
[0027] A preparation method of environment-friendly colored pavement binder, specifically comprising the following steps:
[0028] (1) take each component raw material by weight percentage, for subsequent use;
[0029] (2) Put the environment-friendly aromatic oil into the reactor, and when heated to 150-170°C, add hydrogenated petroleum resin and terpene resin in turn, stir for 50-70min, maintain the temperature at 150-170°C, and stir at a speed of 600- 800rpm / min;
[0030] (3) Add styrene-butadiene rubber and SBS to the liquid after the reaction in step (2), continue to stir and swell for 20-40min, maintain the temperature at 150-170°C, and stir at a speed of 600-800rpm / min;
[0031] (4) Add oil-based color paste to the liquid after the swelling in step (3) is completed, and continue to stir for 20-30 minutes, the temperature is maintained at 150-170° C., and the stirring speed is 600-800 rpm / min;
[0032] (5) Add an antioxidant to the liquid after the reaction in step (4)...
Embodiment 1-5
[0035] The raw materials of each component were weighed according to the weight percentage in Table 1.
[0036] Table 1: each component weight percent (unit: %) of embodiment 1-5
[0037]
[0038]
[0039] According to the ratios and dosages proposed in the weight percentage scheme of each component raw material in Examples 1-5, the color binder was prepared by the same preparation method as above, and the performance test was carried out, as shown in Table 2.
[0040] The detection result of table 2 embodiment 1-5
[0041]
[0042]
[0043] It can be seen from Table 2 that based on the blending ratio and processing technology of the aforementioned components, the products of each example are better than the standard requirements of JTG F40-2019 for road petroleum ordinary asphalt, and most of them meet the requirements of JTG F40-2019 for polymer Standard requirements for modified asphalt. From the experimental data, it can be seen that the penetration index PI,...
Embodiment 6
[0045] A preparation method of environment-friendly colored pavement binder, specifically comprising the following steps:
[0046] (1) take by weighing each component raw material of weight percentage described in embodiment 3, for subsequent use;
[0047] (2) Put the environmentally friendly aromatic oil into the reactor, and when heated to 150°C, add hydrogenated petroleum resin and terpene resin in turn, stir for 50 minutes, keep the temperature at 150°C, and the stirring speed is 600rpm / min;
[0048] (3) Add styrene-butadiene rubber and SBS to the liquid after the reaction in step (2), continue to stir and swell for 20 minutes, maintain the temperature at 150° C., and stir at a speed of 600 rpm / min;
[0049] (4) Add oil-based color paste to the liquid after the swelling in step (3) is completed, and continue to stir for 20 minutes, the temperature is maintained at 150 ° C, and the stirring speed is 600 rpm / min;
[0050](5) Add an antioxidant to the liquid after the reacti...