A manufacturing method and metal mixing technology, applied in the field of fishing equipment, can solve the problems of decreased fishing success rate, wasted time, and skewed swimming posture, and achieve the effects of reducing the probability of attacking lead sinkers, being convenient to use, and maintaining a stable state.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0027] Example 1: A mixed-metal counterweight, which is formed by mixed injection molding of tungsten oxide powder and high molecular polymer, the main composition of the mixed-metal counterweight is: 50% tungsten oxide powder, 45% ethylene raw material %, 5% is plasticizer, the manufacture method of this mixed metal balance weight, comprises the steps:
[0028] a) Select 500g of tungsten oxide powder, grind it with a grinder, and sieve it with a 65-mesh sieve, mainly select tungsten oxide powder with a range of less than 5 μm;
[0029] b) First add 450g of ethylene raw material and 50g of plasticizer to the storage tank, the drying temperature is 80°C, the mass of tungsten oxide powder is 50% of the total mass of the mixture, heat the mixture to 250°C, and then add tungsten oxide powder Stir and mix for 5 minutes, the pouring system injects the pre-mixture into the cavity, the shape of the cavity is the shape of a worm head, hot-pressed, cooled and condensed to make a mixed m...
Embodiment 2
[0030] Example 2: A mixed metal counterweight is formed by mixed injection molding of tungsten oxide powder and high molecular polymer. The main composition of the mixed metal counterweight is: 60% of tungsten oxide powder, 35% of silica gel raw material % and 5% vulcanizing agent, the manufacture method of this mixed metal counterweight, comprises the steps:
[0031] Select 600g of tungsten oxide powder, grind it with a grinder, and sieve it with a 65-mesh sieve, mainly select tungsten oxide powder with a range below 5 μm;
[0032] First add 350g of silica gel raw material and 50g of vulcanizing agent into the storage tank, the drying temperature is 80°C, the mass of tungsten oxide powder is 60% of the total mass of the mixture, heat the mixture to 250°C, then add tungsten oxide powder and stir and mix for 3 minute,
[0033] Inside the mixing cavity, the main body block 12 made of silica gel injection molding is first placed, and then the gating system injects the pre-mixtur...
Embodiment 3
[0034] Embodiment 3: A mixed metal lure is formed by mixed injection molding of tungsten oxide powder and high molecular polymer. The main composition of the mixed metal lure is: 30% of tungsten oxide powder, 65% of silica gel raw material and 5% vulcanizing agent, the manufacture method of this mixed metal lure, comprises the steps:
[0035] Select 300g of tungsten oxide powder, grind it with a grinder, and sieve it with a 65-mesh sieve, and mainly select tungsten oxide powder with a range of less than 5 μm;
[0036] First add 300g of silica gel raw material and 25g of vulcanizing agent to the storage tank, the drying temperature is 80°C, heat the mixture to 250°C, then add tungsten oxide powder and stir for 4 minutes, inject it into the first cavity, and cool and condense as a whole A mixed metal counterweight is made, and the mixed metal counterweight is in the shape of a worm's head.
[0037] Put the mixed metal weight block as the main body in the second cavity, and add ...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More - R&D
- Intellectual Property
- Life Sciences
- Materials
- Tech Scout
- Unparalleled Data Quality
- Higher Quality Content
- 60% Fewer Hallucinations
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2025 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com