Wool and cashmere large biological fiber containing cocoa active ingredients and preparation method thereof
A technology of active ingredients and biological fibers, applied in the field of large biological fibers, can solve the problems of low fragrance, no plant active ingredients, antibacterial properties, low comfort and low permeability, and achieve high permeability, good application prospects, and applications. wide range of effects
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Image
Examples
Embodiment 1
[0029] see figure 1 , the present invention provides the following technical solutions:
[0030] The preparation method of the wool macrobiological fiber containing cocoa active ingredient comprises the following steps:
[0031] S1: preparing an active agent containing cocoa active ingredients;
[0032] S2: Add water at 45°C to the mixing tank, then put the wool fiber into the mixing tank, the weight ratio of water to wool fiber is 30:3.5, then add the active agent prepared in step S1 into the water, and keep the temperature constant Stir for 30min, the weight portion of the wool fiber is: 10 parts, the weight portion of the active agent is: 1 part,
[0033] S3: Warm up the water to 80°C at a rate of 5°C / min, keep stirring at a constant temperature for 1-2 hours and then stop. After the water temperature is naturally cooled to 40°C, remove the wool fiber and perform color-fixing treatment; preferably, Select a dilute solution with a concentration of 3% to fix the wool fiber...
Embodiment 2
[0043] The preparation method of the wool macrobiological fiber containing cocoa active ingredient comprises the following steps:
[0044] S1: preparing an active agent containing cocoa active ingredients;
[0045] S2: Add water at 50°C to the mixing tank, then put the wool fiber into the mixing tank, the weight ratio of water to wool fiber is 30:4, then add the active agent prepared in step S1 into the water, and keep the temperature constant Stir for 35min, the weight portion of the wool fiber is: 15 parts, the weight portion of the active agent is: 1.5 parts,
[0046] S3: Warm up the water to 85°C at a rate of 5°C / min, keep stirring at a constant temperature for 1-2 hours and then stop. After the water temperature is naturally cooled to 40°C, remove the wool fibers and perform color-fixing treatment; preferably, Select a dilute solution with a concentration of 3% to fix the wool fiber, which is not easy to chemically react with the wool fiber and is not easy to cause damag...
Embodiment 3
[0050] The preparation method of the wool macrobiological fiber containing cocoa active ingredient comprises the following steps:
[0051] S1: preparing an active agent containing cocoa active ingredients;
[0052]S2: Add water at 55°C to the mixing tank, then put the wool fiber into the mixing tank, the weight ratio of water to wool fiber is 30:4.5, then add the active agent prepared in step S1 into the water, and keep the temperature constant Stir for 40min, the weight portion of wool fiber is: 20 parts, the weight portion of active agent is: 2 parts,
[0053] S3: Warm up the water to 90°C at a rate of 5°C / min, keep stirring at a constant temperature for 1-2 hours and then stop. After the water temperature is naturally cooled to 40°C, remove the wool fiber and perform color-fixing treatment; preferably, Select a dilute solution with a concentration of 3% to fix the wool fiber, which is not easy to chemically react with the wool fiber and is not easy to cause damage to the w...
PUM
Login to View More Abstract
Description
Claims
Application Information
Login to View More 