A technology for treating chemicals and oil sludge, which is applied in the field of preparation of oil sludge treatment chemicals, can solve problems such as difficult to handle, difficult to separate and remove, and affect treatment efficiency, so as to achieve high sludge treatment efficiency, improve organic effect, and improve treatment effect Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0027] The preparation method of a kind of oil sludge treatment agent of the present embodiment comprises the following steps:
[0028] S1: Preparation of modified cyclodextrin: send cyclodextrin into the modified solution for modification and stirring treatment, the modification speed is 100r / min, the modification time is 30min, the modification temperature is 60°C, and then turn to Stir in the organic agent at high speed for 20 minutes, the high-speed stirring speed is 600r / min, after the stirring is completed, the modified cyclodextrin is obtained;
[0029] S2: Organic treatment of nano jiaoling stone: put nano jiaoling stone into the coupling agent KH560 for low-speed stirring, low speed stirring 50r / min, stirring time 30min, stirring temperature 50°C, after stirring, then wash with water , drying, to obtain organic nano gellingite;
[0030] S3: Hybrid rectorite: send rectorite into the dispersion liquid for stirring and dispersing, the stirring temperature is 70°C, the s...
Embodiment 2
[0044] The preparation method of a kind of oil sludge treatment agent of the present embodiment comprises the following steps:
[0045] S1: Preparation of modified cyclodextrin: send cyclodextrin into the modified liquid for modification and stirring treatment, the modification speed is 500r / min, the modification time is 40min, the modification temperature is 100°C, and then Stir in the organic agent at high speed for 30 minutes, the high-speed stirring speed is 1200r / min, after the stirring is completed, the modified cyclodextrin is obtained;
[0046] S2: Organic treatment of nano jiaolingite: put nano jiaolingite into coupling agent KH560 for low-speed stirring, low-speed stirring 100r / min, stirring time 40min, stirring temperature 100°C, after stirring, then wash with water , drying to obtain organic nano-collite;
[0047] S3: Hybrid rectorite: Put the rectorite into the dispersion liquid for stirring and dispersing, the stirring temperature is 100°C, the stirring time is ...
Embodiment 3
[0061] The preparation method of a kind of oil sludge treatment agent of the present embodiment comprises the following steps:
[0062] S1: Preparation of modified cyclodextrin: send cyclodextrin into the modification solution for modification and stirring treatment, the modification speed is 300r / min, the modification time is 35min, the modification temperature is 80°C, and then turn to Stir in the organic agent at high speed for 25 minutes, the high-speed stirring speed is 900r / min, after the stirring is completed, the modified cyclodextrin is obtained;
[0063] S2: Organic treatment of nano jiaoling stone: put nano jiaoling stone into the coupling agent KH560 for low-speed stirring, low speed stirring 75r / min, stirring time 35min, stirring temperature 75°C, after stirring, then wash with water , drying to obtain organic nano-collite;
[0064] S3: Hybrid rectorite: Put the rectorite into the dispersion liquid for stirring and dispersing, the stirring temperature is 85°C, th...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com