A release agent and decorative board technology, which is applied in sound insulation, petroleum industry, building components, etc., can solve the problems of affecting product quality and export earnings, increasing cost of mineral wool board, high cost, etc., so as to save animal oil resources and reduce production Low cost and good demoulding effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0011] Release agent components: stearic acid 2, castor oil sulfate 1.2, fatty alcohol polyoxyethylene ether sodium sulfate (AES) 1.8, water-soluble silicone oil 0.8, polyacrylamide 0.4, urea 6, pentaerythritol 1.6, metal surface protection agent ( YZ140 (produced in Shanghai) 0.3, EDTA 0.6, appropriate amount of essence, and the balance of water.
[0012] Preparation method: Pour water into the reaction kettle, heat up to 60-95°C, add stearic acid and start the mixer at the same time, stir for 20 minutes, add castor oil sulfate and metal surface protection agent, stir for 20 minutes, then add fatty alcohol poly Sodium oxyethylene ether sulfate, water-soluble silicone oil, polyacrylamide, urea, pentaerythritol, EDTA, stir for 40 minutes, stop heating, add an appropriate amount of essence when cooling to room temperature, stir for 10 minutes, measure, and pack.
Embodiment 2
[0014] Release agent components: stearic acid 1, castor oil sulfate 0.5, fatty alcohol polyoxyethylene ether sodium sulfate 0.9, water-soluble silicone oil 0.3, polyacrylamide 0.1, urea 2, pentaerythritol 0.8, metal surface protection agent 0.2, EDTA 0.4 , the right amount of essence, the balance of water.
[0015] Preparation method: with embodiment 1.
Embodiment 3
[0017] Release agent components: stearic acid 1.5, castor oil sulfate 0.8, fatty alcohol polyoxyethylene ether sodium sulfate 1.5, water-soluble silicone oil 0.5, polyacrylamide 0.2, urea 4, pentaerythritol 1.0, metal surface protection agent 1.5, EDTA 0.5 , the right amount of essence, the balance of water.
[0018] Preparation method: with embodiment 1.