Embodiment 1
[0084] Spherical phenolic resin (particle size = 10 to 700 μm: trade name “High Performance True Spherical Resin Marlin HF500 Type”; manufactured by Qunyei Chemical Co., Ltd.) was sieved with a 250 μm sieve to remove fine powder, and the removed Put 150 g of micropowdered spherical phenol resin into a vertical reaction tube made of quartz with an orifice plate, raise the temperature to 350°C for 1.5 hours under nitrogen flow, and then raise the temperature to 900°C for 6 hours, then keep it at 900°C for 1 hours, 68.1 g of spherical carbonaceous materials were obtained. Subsequently, activation treatment was performed at 900° C. under a mixed gas atmosphere of nitrogen (3 NL / min) and water vapor (2.5 NL / min). When the packing density of spherical activated carbon was reduced to 0.5mL / g, the activation treatment was terminated to obtain 29.9 g of spherical activated carbon (yield 19.9 wt%).
[0085] The characteristics of the obtained spherical activated carbon are shown in Tab...
Embodiment 2
[0087] Instead of the phenolic resin used in Example 1 ( Qun Rong Chemical Co., Ltd.), all the other repeat the method described in Example 1 to obtain spherical activated carbon. The yield was 26.5%.
[0088] The characteristics of the obtained spherical activated carbon are shown in Table 1 and Table 2.
Embodiment 3
[0090] The spherical activated carbon obtained in Example 1 is subjected to an oxidation treatment at 470° C. for 3 hours and 15 minutes through a fluidized bed under a mixed gas atmosphere of nitrogen and oxygen with an oxygen concentration of 18.5 vol%, and then again in a fluidized bed under a nitrogen atmosphere. At 900°C for 17 minutes, reduction treatment was performed to obtain surface-modified spherical activated carbon.
[0091] The characteristics of the obtained surface-modified spherical activated carbon are shown in Table 1 and Table 2.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com