Embodiment 1
[0027] The specification (type) of dry-mixed mortar is mortar for the ground, and the matching standard is to design the ratio of dry sand and cement to 2.6:1 weight percent. The above cement is mixed with cement when the entire cement is regarded as 100 weight percent. 68% by weight, 14% by weight of fly ash, and 18% by weight of expansion agent.
[0028] That is, 720kg of dry sand, 190kg of cement, 40kg of fly ash, and 50kg of expansion agent are mixed into each ton (TON) of dry-mixed mortar, and then 0.02kg of thickener is mixed as an additive, and beneficial microorganisms are added after replacing water. That is, the actual amount of water used is 112-157 kg minus the mixed amount of beneficial microorganisms (13-18 kg).
[0029] The total amount of water used in each ton (TON) of dry-mixed mortar is 125-175kg, and then mixed with 13-18kg of beneficial microorganisms, and poured after mixing with each other. That is, the actual amount of water used is 112-157 kg minus th...
Embodiment 2
[0036] The specification (type) of the dry-mixed mortar is ordinary plastering mortar, and the matching standard is to design the ratio of dry sand and cementing material to 2.6:1. The above-mentioned cementing material is regarded as 100% by weight of the entire cementing material It is formed by mixing 93% by weight of cement and 7% by weight of fly ash.
[0037] That is, 720kg of dry sand, 260kg of cement, and 20.0kg of fly ash are mixed into each ton (TON) of dry-mixed mortar, and then 0.133kg of thickener is mixed as an admixture, and finally water and the total amount of water are added before pouring on site 10% of beneficial microorganisms.
[0038] The total amount of water used in each ton (TON) of dry-mixed mortar is 125-175kg, and the amount of mixed beneficial microorganisms is 13-18kg, which are poured after being mixed with each other. At this time, the amount of water used is 112-157 kg minus the total amount of mixed beneficial microorganisms.
[0039] Table...
Embodiment 3
[0045] The specification (type) of dry-mixed mortar is to choose the mortar for spraying, and the matching standard is to design the ratio of dry sand material and cementing material to 1.5:1, and the cementing material is to mix 63 weight percent of cement when the whole cementing material is regarded as 100 weight percent , 32% by weight of fly ash, 5% by weight of expansion agent, and 3.7% by weight of admixture. That is, the cement is a mixture of cement, fly ash, expansion agent, and admixture.
[0046] Mix 600kg of dry sand, 252kg of cement, 128kg of fly ash, 20kg of expansion agent, and 14.8kg of admixture in each ton (TON) of dry-mixed mortar, and then add water and 10% by weight of the total 100% by weight of water on site of beneficial microorganisms.
[0047] The total amount of water used in each ton (TON) of dry-mixed mortar is 175-225kg, and then the water is replaced to mix 18-23kg of beneficial microorganisms. That is, the actual amount of water used is 157-2...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com