Environment-protective type plant cover concrete
An environmentally friendly technology for planting concrete, applied in the direction of sustainable waste treatment, solid waste management, climate sustainability, etc., can solve the problems of destroying the ecological environment and the impact of waste concrete on the ecological environment, and achieve the effect of convenient construction and high strength
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0015] (1) Crushing waste concrete as waste concrete aggregates requires a crushing value of less than 30%, a mud content of less than 2%, and a single gradation of particle size of 5mm;
[0016] (2) Amorphous silicon dioxide (SiO 2 ) 67 parts, 30 parts of zeolite, 3 parts of acidic plant extract (for commercially available products, such as the hawthorn extract produced by Shaanxi Senfu Biotechnology Co., Ltd.) mixed to make concrete alkaline neutralizer
[0017] (3) Mix 84kg of water, 300kg of ordinary portland cement with a grade of not less than 52.5, 1500kg of waste concrete aggregate in step (1), 30kg of concrete alkaline neutralizer in step (2) and polycarboxylate superplasticizer 3kg mixed and stirred evenly with a mixer;
[0018] (4) Pouring and pounding the prefabricated mold with the stirred material;
[0019] (5) Carry out maintenance, maintenance condition: temperature is 20 ℃, and humidity is 50%;
[0020] (6) After the mold is removed, it is the finished prod...
Embodiment 2
[0022] (1) Crushing waste concrete as waste concrete aggregate requires a crushing value of less than 30%, a mud content of less than 2%, and a particle size of 38mm in a single gradation;
[0023] (2) Mix 71 parts of amorphous silica, 28 parts of zeolite, and 1 part of acid plant extract to make concrete alkaline neutralizer
[0024] (3) Mix 160kg of water, 500kg of ordinary portland cement with a grade of not less than 52.5, 2500kg of waste concrete aggregate in step (1), 100kg of concrete alkaline neutralizer in step (2) and polycarboxylate superplasticizer Mix 10kg and stir evenly with a mixer;
[0025] (4) Pouring and pounding the prefabricated mold with the stirred material;
[0026] (5) Carry out maintenance, maintenance condition: temperature is 20 ℃, and humidity is 50%;
[0027] (6) After the mold is removed, it is the finished product.
Embodiment 3
[0029] (1) Crushing waste concrete as waste concrete aggregate requires a crushing value of less than 30%, a mud content of less than 2%, and a particle size of 22mm in a single gradation;
[0030] (2) 69 parts of amorphous silicon dioxide, 29 parts of zeolite, and 2 parts of acid plant extract are mixed to make concrete alkaline neutralizer;
[0031] (3) Mix 102kg of water, 340kg of ordinary portland cement whose grade is not less than 52.5, 1700kg of waste concrete aggregate in step (1), 51kg of concrete alkaline neutralizer in step (2) and polycarboxylate superplasticizer Mix 5.1kg and stir evenly with a mixer;
[0032] (4) Pouring and pounding the prefabricated mold with the stirred material;
[0033] (5) Carry out maintenance, maintenance condition: temperature is 20 ℃, and humidity is 50%;
[0034] (6) After the mold is removed, it is the finished product.
PUM
Property | Measurement | Unit |
---|---|---|
strength | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
particle diameter | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com