Embodiment 1
[0021] A kind of composite material for outdoor lighting of the present invention, it comprises: EPM calculated by weight percentage 2 45% of ion resin, 3% of adhesive paint material, 1.5% of antioxidant and ultraviolet absorber, 45% of active nano-calcium carbonate, 5% of fireproofing agent, 0.25% of liquid dispersant and 0.25% of lubricant E wax.
[0022] Among them, the special adhesive paint material can greatly improve the adhesion of the product to the paint; the antioxidant and ultraviolet absorber can improve the outdoor aging resistance of the product; the special nano-scale reinforced mineral powder is used to reduce the cost, improve the hardness of the material, and beautify the surface of the material; Fire retardants are used to reduce the flammability of materials.
[0023] The fire retardant is polytetrafluoroethylene powder.
[0024] The antioxidant is antioxidant KY7910.
[0025] Described ultraviolet absorber is ultraviolet absorber UV531.
[0026] The li...
Embodiment 2
[0032] A kind of preparation method of composite material for outdoor lamps of embodiment 1, it is to calculate by weight percentage ionic resin 45%, polytetrafluoroethylene powder 5%, active nano-calcium carbonate 45%, special-purpose adhesion paint material CA- 13%, additive 1 (liquid dispersant MFA 0.25%), additive 5 (antioxidant KY7910 0.5%), additive 6 (antioxidant 168 0.5%), additive 7 (ultraviolet absorber UV531 0.5%) , Auxiliary 8 (microcrystalline wax lubricant E wax 0.25%) is added to the high-speed extruder, the temperature of the extruder is controlled between 180--215 degrees Celsius, the screw speed of the extruder is 380r / min., and it comes out of the extruder Promptly obtain the composite material for lamps and lanterns of embodiment 1 afterwards.