Water-based paint remover as well as preparation method and using method thereof
A paint remover and water-based technology, which is applied in the field of water-based paint remover and its preparation, can solve the problems of large environmental pollution and high cost of paint remover, and achieve cost-friendly, pollution-free, strong paint-removing ability and low cost Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
preparation example Construction
[0019] In the preparation method of the water-based paint remover of the present invention, wherein the sodium hydroxide and the alkali auxiliary agent are completely dissolved, and then the composite additive and the washing agent are added in sequence. After the composite additives and builders are added into the solution, the temperature of the solution is raised to 60-70° C., and the oxidizing agent is slowly added, and evenly stirred to completely dissolve each component.
[0020] When using the water-based paint remover of the present invention, the paint remover is directly put into the paint remover and soaked. Generally, it is preferred to heat the paint remover to 75-85° C. for soaking, which can reduce the paint removal time. After soaking, wash the paint-removing parts with water, then acid-wash the paint-removing parts to make the paint film swell and fall off, and finally wash with water. The paint-removing time is generally 8-100 minutes.
Embodiment 1
[0022] Sodium hydroxide 100g / L, alkali additive 120g / L, potassium permanganate 40g / L, composite additive 15g / L, sodium citrate 1.0g / L, wherein the alkali additive is a mixture of sodium carbonate and trisodium phosphate, The composite additive is a compound composed of sodium metasilicate: sodium benzenesulfonate at a ratio of 1:0.05.
[0023] Add sodium hydroxide and alkali additives to the water in turn. After they are completely dissolved, add compound additives and sodium citrate in turn, and then heat up to 70°C, then slowly add potassium permanganate. The whole process is under the condition of constant stirring After the solid solute is completely dissolved, it can be put into the paint-removing parts. The paint-removing parts are soaked in the paint remover at a temperature of 85°C, and then washed-acid-washed. The paint-removing time is 90-100 minutes. The rate can reach 100%.
Embodiment 2
[0025] Sodium hydroxide 80g / L, trisodium phosphate 100g / L, potassium permanganate 40g / L, composite additive 8g / L, potassium citrate 0.5g / L, wherein said composite additive is sodium silicate: triethanolamine is A compound composed of a ratio of 1:0.1.
[0026] Add sodium hydroxide and trisodium phosphate to the water in turn. After completely dissolving, add compound additives and potassium citrate in turn, and then heat up to 65°C, then slowly add oxidant. The whole process is carried out under the condition of constant stirring. After the solid solute is completely dissolved, it can be put into the paint-removing parts. The paint-removing parts are soaked in the paint remover at a temperature of 85°C, and then washed-acid-washed. The paint-removing time is 70-90 minutes, and the paint-removing rate It can reach 100%. The type of paint film is an electrophoretic epoxy resin paint film with a thickness of 15-25 μm, and an epoxy paint with a thickness of 20-45 μm is sprayed.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com