Environment-friendly modified chlorinated polypropylene adhesive and preparation method thereof
A chlorinated polypropylene, environmentally friendly technology, used in adhesives, graft polymer adhesives, adhesive types and other directions, can solve problems such as toxic solvents, and achieve good adhesion, high cost performance and simple preparation process. Effect
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Add 100 parts by weight of chlorinated polypropylene (CPP), 25 parts by weight of maleic anhydride and 300 parts by weight of methylcyclohexane into a reactor with a stirring device, heat up to 80°C under stirring, and wait for CPP, After the monomers were completely dissolved, 5 parts by weight of dibenzoyl peroxide was added, and then the temperature was raised to 100°C. After reacting for 3 hours, stop heating, precipitate the product with acetone, then suction filter it with a Buchner funnel, dissolve it with 200 parts by weight of methylcyclohexane after drying, and add 10 parts by weight of petroleum resin to prepare an environmentally friendly modified product. chlorinated polypropylene adhesive.
Embodiment 2
[0020] Add 100 parts by weight of chlorinated polypropylene (CPP), 10 parts by weight of maleic anhydride, 10 parts by weight of butyl acrylate, 150 parts by weight of methylcyclohexane and 150 parts by weight of butyl acetate into a reactor with a stirring device During heating, the temperature was raised to 80°C under stirring, and after the CPP and monomers were completely dissolved, 5 parts by weight of dibenzoyl peroxide was added, and the temperature was raised to 100°C. After reacting for 3 hours, stop heating, precipitate the product with acetone, then suction filter it with a Buchner funnel, dissolve it with 100 parts by weight of methylcyclohexane and 100 parts by weight of butyl acetate after drying, and add 10 parts by weight of rosin resin The environment-friendly modified chlorinated polypropylene adhesive can be prepared.
Embodiment 3
[0022] 100 parts by weight of chlorinated polypropylene (CPP), 5 parts by weight of maleic anhydride, 10 parts by weight of N, N-dimethacrylic acid amide, 10 parts by weight of butyl acrylate, 150 parts by weight of methylcyclohexane and butyl acetate Add 150 parts by weight of ester into a reactor equipped with a stirring device, and heat up to 80°C under stirring. After the CPP and monomers are completely dissolved, add 5 parts by weight of dibenzoyl peroxide, and then raise the temperature to 100°C. After reacting for 3 hours, stop heating, use acetone to precipitate the product, then use a Buchner funnel to suction filter, and after drying, dissolve it with 100 parts by weight of methylcyclohexane and 100 parts by weight of butyl acetate, and add 10 parts by weight of petroleum resin. The environment-friendly modified chlorinated polypropylene adhesive can be prepared.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com