Processing method for improving abrasion resistance of ironing-free shirt ready-made clothes
A processing method and a wear-resistant technology, applied in heating/cooling fabrics, textiles and papermaking, fabric surface trimming, etc., can solve the problems of reducing the service life of non-iron shirts, affecting the durability of shirts, and easily being worn by shirts , to achieve the effect of good heat insulation, improved protection effect and low processing cost
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0010] Example 1: The shirt garment made from the 80S / 2×80S / 2 cotton shirting fabric treated with liquid ammonia using compact spinning yarn as the raw material is used as the test object, and the subsequent finishing process is as follows:
[0011] (1), wash the shirt garment with clean water, and dehydrate and dry;
[0012] (2), the shape memory modified 2D non-ironing resin finishing solution with a prepared concentration of 100g / L is evenly sprayed on the shirt garment by an atomizing sprayer;
[0013] (3) Dry the ready-made shirt garment sprayed with the non-ironing resin finishing solution in the dryer until the moisture content is about 60%, and take it out after being cooled by cold air;
[0014] (4) Put the ready-made shirt into the pressing mold for high-temperature and high-pressure pressing to form it, and after pressing and flattening, hang the ready-made garment on the shelf;
[0015] (5) Take a semi-closed heat shield with one end open, put the heat shield on t...
Embodiment 2
[0020] Example 2: The shirt garment made of 100S / 2×100S / 2 cotton shirting fabric treated with liquid ammonia using compact spinning yarn as the raw material is used as the test object, and the subsequent finishing process is basically the same as that of Example 1. The same, except that the concentration of the 2D no-ironing resin finishing solution in step (2) is 80 g / l, and the high-temperature baking condition in step (5) is baking at 130° C. for 6 minutes.
[0021] The washing test was carried out on the non-iron shirts treated by the above method. After washing 5 times, the cloth surface grade of the garments was 4.0. After washing and drying 50 times, the collar and cuffs of the shirts that were most likely to be worn out were still intact and undamaged , the other parts of the shirt were also intact, and the destructive test was continued. After 61 washes, the collar tip and cuff edge of the shirt were damaged. And the non-ironing shirt ready-made garment that does not ...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com