A technology of dental arch wire and metal, which is applied in the field of preparation of stealth coating on the surface of metal dental arch wire for orthodontics, can solve the problems of affecting the appearance and affecting the physical and mental health of young people, and achieves the effect of simple preparation method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
specific Embodiment approach 1
[0015] Specific implementation mode 1: The preparation method of the stealth coating on the surface of the metal dental arch wire for orthodontics in this embodiment is realized through the following steps: (1) pretreatment of the surface of the metal dental arch wire; (2) applying the pretreated dental arch wire to The mold is straightened and fixed, and put into the dipping solution for lifting coating; (3) The coated dental arch wire is left at a clean room temperature for 15 minutes, and cured at a high temperature to obtain a stealth coated metal dental arch wire. Wherein step (2) described dip coating solution is the mixed solution of aqueous polyurethane emulsion and White-6 white slurry, polyurethane emulsion and white slurry ratio are 4:1~6:1, add distilled water to make the viscosity of dip coating solution be coating -4 cups, about 1 minute to 1 minute and 30 seconds.
[0016] The present invention can directly dip-coat the surface of the metal dental arch wire for ...
specific Embodiment approach 2
[0018] Embodiment 2: The difference between this embodiment and Embodiment 1 is that the metal arch wire in step (1) can be a NiTi alloy arch wire or a stainless steel arch wire. Other steps and selected parameters are the same as those in Embodiment 1.
specific Embodiment approach 3
[0019] Embodiment 3: The difference between this embodiment and Embodiment 1 is that the pretreatment in step (1) is ultrasonic cleaning in acetone, alcohol, and distilled water for more than 10 minutes to remove oil stains. Other steps and selected parameters are the same as those in Embodiment 1.
PUM
Property | Measurement | Unit |
---|---|---|
hardness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
thickness | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com