A preparation method, polymer technology, applied in the direction of drilling composition, chemical instruments and methods, etc., can solve the problems of high labor intensity of operators, waste of polymers, high energy consumption, etc., and reduce adverse health factors , The error of the preparation concentration is small, and the effect of eliminating the degradation of oxygen exposure
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0021] Take 80-150 mesh, 50 parts by weight of Baomo polyacrylamide dry powder in a beaker, add 40 parts by weight of a mixture of alcohol: glycerol, ethylene glycol, and isopropanol in a weight ratio of 1 : 2:12, after stirring evenly at a stirring speed of 70 rpm, under continuous stirring, sequentially add 20 parts by weight of Tween 80, 20 parts by weight of 15# white oil, and 10 parts by weight The silica bath soil, at the above-mentioned stirring speed, continued to stir for 1 hour to obtain 140 parts by weight of the suspended polymer.
Embodiment 2
[0023] Take 40 parts by weight of 80-150 mesh polyacrylamide dry powder in the reactor, add 30 parts by weight of mixed alcohol: glycerol, ethylene glycol, and isopropanol in a weight ratio of 1: 2:12. After stirring evenly at a stirring speed of 70 rev / min, under continuous stirring, successively add 15 parts by weight of Tween 80, 15 parts by weight of 15# white oil, and 5 parts by weight of sodium dihydrogen phosphate. At the above stirring speed, the stirring was continued for another 0.5 hour to obtain 105 parts by weight of suspended polymer.
Embodiment 3
[0025] Take 30 parts by weight of 80-150 mesh pre-crosslinked gel dry powder in the reactor, add 20 parts by weight of mixed alcohol: glycerol, ethylene glycol, and isopropanol in a weight ratio of 1:2 : 12, after the stirring speed of 70 rev / min is even, continue to stir and add successively the Tween 80 that is 10 parts by weight, the 15# white oil that the weight part is 10 parts, under above-mentioned stirring speed, continue to stir again 1.2 Hours, 70 parts of suspended polymer were obtained.
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com