Halogen-free anti-buckling-deformation reinforced nylon 6 and manufacturing process thereof

A production process and anti-warping technology, which is applied in the field of organic polymer composite materials, can solve problems such as warping and deformation of finished products, troubles of export enterprises, and large internal stress, and achieve convenient production and procurement, good anti-warping deformation, and improved The effect of comprehensive competitiveness

Inactive Publication Date: 2013-01-23
KECHUANG POLYMER SUZHOU
View PDF1 Cites 3 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

Therefore, it has caused serious troubles to many export enterprises in my country.
At the same time, because glass fiber has a large aspect ratio, and nylon 6 is a crystalline material, it is easy to generate large internal stress during molding, resulting in warping and deformation of the finished product
[0003] At present, there are already anti-warping reinforced nylon 6 materials in the market, which use talcum powder to prevent warping, which has a series of disadvantages such as low strength, insufficient anti-warping effect, affecting the appearance of the product, and poor fluidity of the material.

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0010] Embodiment 1 provides a halogen-free anti-warping and deformation-reinforced nylon 6, which is composed of the following components by weight: nylon 6: 48%, nylon 6 carrier high-pigment black masterbatch: 1.5%; halogen-free and alkali-free glass fiber: 23% %; Halogen-free glass beads: 22%: toughening agent: 3%; coupling agent: 0.3%; other additives: 2.2%;

[0011] Dry nylon 6 first, and then weigh the dried nylon 6, nylon 6 carrier high-pigment black masterbatch, halogen-free glass beads, toughening agent, coupling agent, and other additives in the mixer according to the proportion Mix at low speed for 10 minutes, the mixer adopts low speed mixing, the gap between the mixing blade and the cylinder wall should be less than 0.5 cm, the mixing effect of raw and auxiliary materials should be visually observed that the various particles and powders are basically uniform, and there is no obvious agglomerate or agglomeration; twin-screw extruder Use 36 length-to-diameter ratio...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention relates to an organic high polymer composite material, and more specifically relates to a halogen-free anti-buckling-deformation reinforced nylon 6 and a manufacturing process thereof. The halogen-free anti-buckling-deformation reinforced nylon 6 is composed of the following components in percentage by weight: 45-70% of nylon 6, 1-35% of halogen-free and alkali-free glass fiber, 1-40% of halogen-free glass microsphere, 1-5% of toughener, 0.1-0.4% of coupling agent and 0.1-5.5% of other assistants. According to the invention, the halogen-free anti-buckling-deformation reinforced nylon 6 and the manufacturing process thereof have the characteristics that the reinforced nylon 6 is halogen-free and environment-friendly and a good anti-buckling-deformation property is added on the basis of keeping favorable comprehensive mechanical properties, thereby being more suitable for the production of masks / shells required to be tightly assembled and molded parts such as product frameworks and the like; and both the production and the procurement are convenient. Thus, the comprehensive competitive power of the product is comprehensively improved.

Description

technical field [0001] The invention relates to an organic polymer composite material, more specifically, relates to a halogen-free anti-warping deformation reinforced nylon 6 and its manufacturing process. Background technique [0002] Nylon 6 is one of the most widely used engineering plastics. Its amide group is polar and has a strong hydrogen bond in its structure, which makes nylon 6 have a high melting point and good physical and mechanical properties. And wear resistance and self-lubricating properties, these comprehensive characteristics are not available in other plastics. However, the heat distortion temperature of pure nylon 6 is low, the water absorption is high, the impact strength before water absorption is low, the rigidity drops sharply after water absorption, and the size is unstable, which limits the application of nylon 6 and further reduces the downstream industry. Material selection for design engineers. Therefore, research on compound modification of ...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Applications(China)
IPC IPC(8): C08L77/02C08K13/04C08K7/14C08K7/20
Inventor 孙平
Owner KECHUANG POLYMER SUZHOU
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products