Production method of environment-friendly fiber colored art paper
A production method and art paper technology, applied in natural cellulose pulp/paper, special paper, fiber raw material processing, etc., can solve the problems of plant fiber without affinity, production and use obstacles, and rigid shape, etc., to achieve a good sense of art and Aesthetics, easy processing and production, and natural paper texture
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0023] Embodiment 1, a kind of production method of off-white environment-friendly fiber color art paper, it comprises the following steps:
[0024] (1) The basic pulp is equipped with 100% commercial bleached kraft chemical wood pulp as raw material, and the selected pulp ratio is 30% of Canadian Kelly softwood pulp and 70% of Rizhao Senbo hardwood pulp. The way of mixing and beating, control the beating degree of pulp beating to 33-35oSR;
[0025] (2) Coniferous wood pulp is used as the raw material for the preparation and dyeing of fiber pulp, and the coniferous wood pulp board is placed in a hydraulic pulper with a crushing concentration of 4-5% and a crushing time of 15-20 minutes. Under the action, the paddle board is crushed into fiber pulp, in which the length of a single fiber is 2~4mm, and the width is 40~60μm. The fiber pulp after the crushing is dyed, and dyeing is added to the hydraulic pulper. After the solid dye is disintegrated and dyed, put it into a storage...
Embodiment 2
[0029] Embodiment 2, a kind of production method of light yellow environment-friendly fiber color art paper, it comprises the following steps:
[0030](1) The basic pulp is equipped with 100% commercial bleached kraft chemical wood pulp as raw material, and the selected pulp ratio is 30% of Canadian Kelly softwood pulp and 70% of Rizhao Senbo hardwood pulp. The way of mixing and beating, control the beating degree of pulp beating to 33-35oSR;
[0031] (2) The preparation and dyeing of fiber pulp. Select coniferous wood pulp as raw material, put the coniferous wood pulp board into 2m 3 In the hydraulic pulper, the crushing concentration is 4-5%, and the crushing time is 15-20 minutes. Under the action of water conservancy and machinery, the paddle boards are crushed into fiber pulp, and the length of a single fiber is 2-4mm, and the width 40~60μm, dye the disintegrated fiber pulp, add solid dye for dyeing into the hydraulic pulper, after the disintegration and dyeing are compl...
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
width | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com