[0024] Below in conjunction with embodiment the present invention will be further described.
[0025] Brown corundum fine powder, polyethylene terephthalate (PET), and 0.3% calcium stearate are mixed in proportions of 5%, 94.7%, and 0.3% calcium stearate. Its production steps are as follows:
[0026] The first step, (1) Polyethylene terephthalate (PET) 94.7%, dried at 140 degrees Celsius under vacuum conditions;
[0027] In the second step, maintain a temperature of 140 degrees Celsius, add 0.3% calcium stearate under normal pressure, and mix well;
[0028] In the third step, add 5% brown corundum powder and mix well;
[0029] In the fourth step, the mixture is melted and extruded by a screw, and then sprayed out through a spinneret for spinning and winding to obtain as-spun filaments;
[0030] In the fifth step, after balancing, stretching, crimping, relaxation and heat setting are performed to obtain polyester polished fiber filaments.
[0031] Brown corundum micropowde...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com