A technology of anti-rust emulsified oil and engine oil, which is applied in the petroleum industry, lubricating compositions, etc., can solve the problems of short anti-rust paint, long anti-rust period of anti-rust oil, and high cost, so as to prolong the anti-rust cycle and emulsify oil The effect of stable system and good emulsification stability

Active Publication Date: 2016-04-20
山西英莱壳科技股份有限公司
View PDF0 Cites 0 Cited by
  • Summary
  • Abstract
  • Description
  • Claims
  • Application Information

AI Technical Summary

Problems solved by technology

The preparation of antirust water is simple and low in cost, but the antirust paint is short and is greatly affected by the weather
The anti-rust oil has a long anti-rust period, but due to the large amount of crude oil used, the cost becomes higher
The emulsified anti-rust oil has the characteristics of the above two products. Surfactants such as triethanolamine oleate are added as emulsifiers. When used, a certain proportion of water is added to the anti-rust oil to form a uniformly dispersed emulsion. , but due to the presence of surfactants, it will absorb moisture in the air through its hydrophilic groups, making the anti-rust period shorter

Method used

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
View more

Image

Smart Image Click on the blue labels to locate them in the text.
Viewing Examples
Smart Image
  • A kind of antirust emulsified oil and preparation method thereof

Examples

Experimental program
Comparison scheme
Effect test

Embodiment 1

[0017] An antirust emulsified oil, comprising by weight components: 10 parts of barium petroleum sulfonate, 3 parts of sodium petroleum sulfonate, 8 parts of sulfonated oil DAH, 2 parts of triethanolamine, 0.5 part of glycerol, 0.2 part of emulsified silicone oil, 5 parts of zinc naphthenate, 2 parts of oleic acid, 1 part of sulfonated oleic acid, 70 parts of No. 10 motor oil.

[0018] The preparation method of antirust emulsified oil described above, prepares according to the following steps:

[0019] (1) Weigh each component according to parts by weight;

[0020] (2) Heat No. 10 engine oil to 80°C, then add barium petroleum sulfonate, sodium petroleum sulfonate, triethanolamine, and zinc naphthenate under the stirring condition of 50 rpm, and stir evenly to obtain a mixed solution;

[0021] (3) Cool the mixture obtained in step (2) to 60°C, add the remaining components, stir evenly at 60 rpm, and cool down to room temperature to obtain the anti-rust emulsified oil.

Embodiment 2

[0023] An anti-rust emulsified oil, comprising by weight components: 12 parts of barium petroleum sulfonate, 4 parts of sodium petroleum sulfonate, 11 parts of sulfonated oil DAH, 3 parts of triethanolamine, 1.2 parts of glycerol, 0.3 parts of emulsified silicone oil, 6 parts of zinc naphthenate, 3 parts of oleic acid, 2 parts of sulfonated oleic acid, 82 parts of No. 10 engine oil.

[0024] The preparation method of antirust emulsified oil described above, prepares according to the following steps:

[0025] (1) Weigh each component according to parts by weight;

[0026] (2) Heat No. 10 engine oil to 80°C, then add barium petroleum sulfonate, sodium petroleum sulfonate, triethanolamine, and zinc naphthenate under the stirring condition of 55 rpm, and stir evenly to obtain a mixed solution;

[0027] (3) Cool the mixture obtained in step (2) to 55°C, add the remaining components, stir evenly at 65 rpm, and cool down to room temperature to obtain the anti-rust emulsified oil.

Embodiment 3

[0029] A kind of antirust emulsified oil, comprising by weight components: 13 parts of barium petroleum sulfonate, 5 parts of sodium petroleum sulfonate, 12 parts of sulfonated oil DAH, 4 parts of triethanolamine, 1.5 parts of glycerol, 0.4 parts of emulsified silicone oil, 8 parts of zinc naphthenate, 4 parts of oleic acid, 3 parts of sulfonated oleic acid, 85 parts of No. 10 engine oil.

[0030] The preparation method of antirust emulsified oil described above, prepares according to the following steps:

[0031] (1) Weigh each component according to parts by weight;

[0032] (2) Heat No. 10 engine oil to 85°C, then add barium petroleum sulfonate, sodium petroleum sulfonate, triethanolamine, and zinc naphthenate under the stirring condition of 56 rpm, and stir evenly to obtain a mixed solution;

[0033] (3) Cool the mixture obtained in step (2) to 56°C, add the remaining components, stir evenly at 65 rpm, and cool down to room temperature to obtain the anti-rust emulsified o...

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

PUM

No PUM Login to view more

Abstract

The invention discloses an antirust emulsified oil and a preparation method thereof. The antirust emulsified oil comprises: 10-15 parts of petroleum barium sulfonate, 3-7 parts of petroleum sodium sulfonate, sulfonated oil DAH? 8-15 parts, 2-6 parts of triethanolamine, 0.5-2 parts of glycerin, 0.2-0.6 parts of emulsified silicone oil, 5-10 parts of zinc naphthenate, 2-6 parts of oleic acid, 1-5 parts of sulfonated oleic acid Parts, 70-90 parts of No. 10 engine oil; the preparation method is to heat No. 10 engine oil to 80-90 ° C, and then add barium petroleum sulfonate, sodium petroleum sulfonate, triethanolamine, and zinc naphthenate under stirring conditions, and stir Evenly, to obtain a mixed solution, then lower the temperature to 50-60°C, add the remaining components, stir evenly, and cool down to room temperature to obtain anti-rust emulsified oil. It is determined that the anti-rust emulsified oil provided by the invention has good emulsification and stability performance, and the anti-rust performance can reach more than 70 days.

Description

technical field [0001] The invention belongs to the technical field of oil preparation for machinery, and in particular relates to an antirust emulsified oil and a preparation method thereof. Background technique [0002] Mechanical parts must be rust-proofed during the manufacturing process. At present, the widely used anti-rust products are anti-rust water, anti-rust oil or emulsified anti-rust oil. The antirust water is simple to prepare and low in cost, but the antirust paint is short and is greatly affected by the weather. The anti-rust oil has a long anti-rust period, but due to the large amount of crude oil used, the cost becomes higher. The emulsified anti-rust oil has the characteristics of the above two products. Surfactants such as triethanolamine oleate are added as emulsifiers. When used, a certain proportion of water is added to the anti-rust oil to form a uniformly dispersed emulsion. , but due to the presence of surfactants, it will absorb moisture in the a...

Claims

the structure of the environmentally friendly knitted fabric provided by the present invention; figure 2 Flow chart of the yarn wrapping machine for environmentally friendly knitted fabrics and storage devices; image 3 Is the parameter map of the yarn covering machine
Login to view more

Application Information

Patent Timeline
no application Login to view more
Patent Type & Authority Patents(China)
IPC IPC(8): C10M169/04C10N30/12C10N40/08
Inventor 求才军
Owner 山西英莱壳科技股份有限公司
Who we serve
  • R&D Engineer
  • R&D Manager
  • IP Professional
Why Eureka
  • Industry Leading Data Capabilities
  • Powerful AI technology
  • Patent DNA Extraction
Social media
Try Eureka
PatSnap group products