A kind of solid spray and preparation method thereof
A solid and weight percentage technology, which is applied in the field of solid spray and solid spray preparation, can solve the problems of uneven spraying and time-consuming, etc., and achieve the effects of excellent moisturizing performance, convenient use and stable system
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0047] Take by weighing the following components (percentage by weight):
[0048] Glycerin 1.00%, Propylene Glycol 1.00%, Xanthan Gum 0.01%, Calcium Chloride Solution (Mass Concentration: 10.00%) 5.00%, Gellan Gum 0.10%, Preservative 0.10%, Natto Gum 0.10%, Sodium Polyglutamate 0.10%, the balance in purified water.
[0049] Prepare the solid spray of the present invention according to the following steps:
[0050] 1. Add gellan gum and xanthan gum to propylene glycol and glycerin in advance to disperse into a uniform slurry,
[0051] 2. Add water, stir and heat to 70-80°C to make the colloid fully hydrated into a uniform solution.
[0052] 3. Slowly add calcium chloride solution while stirring, stir evenly, and then start to cool down.
[0053] 4. When the temperature drops to 50°C, add preservatives, natto gum, and sodium polyglutamate, stir evenly, stop cooling, and wait for the material to cool down to room temperature.
[0054] The solid moisturizing spray obtained in ...
Embodiment 2
[0056] Take by weighing the following components (percentage by weight):
[0057] Glycerin 5.00%, Propylene Glycol 10.00%, Xanthan Gum 0.50%, Calcium Chloride Solution 10.00% (mass concentration 15.00%), Gellan Gum 1.30%, Preservative 0.30%, Natto Gum 0.50%, Sodium Polyglutamate 0.60%, the balance in purified water.
[0058] Method steps:
[0059] 1. Add gellan gum and xanthan gum to propylene glycol and glycerin in advance to disperse into a uniform slurry,
[0060] 2. Add water, stir and heat to 70-80°C to make the colloid fully hydrated into a uniform solution.
[0061] 3. Slowly add calcium chloride solution while stirring, stir evenly, and then start to cool down.
[0062] 4. When the temperature drops to 50°C, add preservatives, natto gum, and sodium polyglutamate, stir evenly, stop cooling, and wait for the material to cool down to room temperature.
[0063] The solid moisturizing spray obtained in this embodiment is a non-flowing solid product, which can be atomize...
Embodiment 3
[0065] Take by weighing the following components (percentage by weight):
[0066] Glycerin 3.00%, Propylene Glycol 5.00%, Xanthan Gum 0.25%, Calcium Chloride Solution (Mass Concentration: 12.50%) 7.50%, Gellan Gum 0.60%, Preservative 0.20%, Natto Gum 0.30%, Sodium Polyglutamate 0.30%, the balance in purified water.
[0067] Method steps:
[0068] 1. Add gellan gum and xanthan gum to propylene glycol and glycerin in advance to disperse into a uniform slurry, then add water, stir and heat to 70-80°C to completely hydrate the colloid into a uniform solution.
[0069] 3. Slowly add calcium chloride solution while stirring, stir evenly, and then start to cool down.
[0070] 4. When the temperature drops to 50°C, add preservatives, natto gum, and sodium polyglutamate, stir evenly, stop cooling, and wait for the material to cool down to room temperature.
[0071] The solid moisturizing sprays of Examples 1 to 3 of the present invention are non-fluid transparent solid products, resis...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com