Wood preservative treatment method
A treatment method and wood preservative technology, applied in the agricultural field, can solve the problems of low treatment efficiency and uniformity of treatment, and achieve the effects of good anti-corrosion treatment effect, good anti-loss performance and high safety.
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0024] 1) Standing tree selection. The tree species of producing anticorrosive wood must select the kind that grows rapidly, and material is better, and present embodiment selects poplar for use, chooses the live poplar tree that branch is less in the above-mentioned tree species, and stem is straight and perfect, without disease and insect damage.
[0025] 2) Sapwood moisture cutting and sealing: The sapwood is sawed at a distance of 20cm from the standing tree to the ground, and the sawing depth is required to be the thickness of the sapwood.
[0026] 3) Heartwood moisture sealing: After the sapwood sawing is completed, the heartwood moisture sealing is carried out, and the new type of liquid paraffin is used to seal the heartwood moisture, and neoprene is injected into the circular area of the sawn sapwood section, and the periphery of the sapwood sawing is made of metal. The rings are reinforced to prevent the trees from being blown down by the wind.
[0027] 4) Prepare...
Embodiment 2
[0033] 1) Standing tree selection. The tree species of producing anti-corrosion wood must select the kind that grows rapidly, and material is better, and present embodiment selects paulownia for use, selects the living poplar tree that branch is few in the above-mentioned tree species, and stem is straight and perfect, without disease and insect pest.
[0034] 2) Sapwood moisture cutting and sealing: The sapwood is sawed at a distance of 20cm from the standing tree to the ground, and the sawing depth is required to be the thickness of the sapwood.
[0035] 3) Heartwood moisture sealing: After the sapwood sawing is completed, the heartwood moisture sealing is carried out, and the new type of liquid paraffin is used to seal the heartwood moisture, and neoprene is injected into the circular area of the sawn sapwood section, and the periphery of the sapwood sawing is made of metal. The rings are reinforced to prevent the trees from being blown down by the wind.
[0036] 4) Prep...
Embodiment 3
[0041] 1) Standing tree selection. The tree species of producing anti-corrosion wood must select the kind that grows rapidly, and material is better, and present embodiment selects Chinese fir, selects the live poplar tree that branch is less in the above-mentioned tree species, and stem is straight and perfect, without disease and insect damage.
[0042] 2) Sapwood moisture cutting and sealing: The sapwood is sawed at a distance of 20cm from the standing tree to the ground, and the sawing depth is required to be the thickness of the sapwood.
[0043] 3) Heartwood moisture sealing: After the sapwood sawing is completed, the heartwood moisture sealing is carried out, and the new type of liquid paraffin is used to seal the heartwood moisture, and neoprene is injected into the circular area of the sawn sapwood section, and the periphery of the sapwood sawing is made of metal. The rings are reinforced to prevent the trees from being blown down by the wind.
[0044] 4) Prepare t...
PUM
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com