Mixed flammable incense and production method thereof
An incense-burning, fully-mixed technology, applied to floor fabrics, household utensils, religious or sacrificial utensils, etc., can solve the problems of easily causing fire hazards, a variety of harmful gases, requiring repeated ignition, etc., to achieve less harm to humans and animals. , The effect of low production cost and simple processing method
- Summary
- Abstract
- Description
- Claims
- Application Information
AI Technical Summary
Problems solved by technology
Method used
Examples
Embodiment 1
[0018] Embodiment 1 Mixed formula and production method of flammable incense
[0019] formula:
[0020] The weight ratio of the ignition material to the main material of the incense is 1:99.
[0021] The composition and parts by weight of the main raw materials for burning incense are: 20 parts of wood powder, 10 parts of elm bark powder, 0.5 part of star anise leaf powder, 0.5 part of orange yellow pigment, and 2 parts of rosin.
[0022] The composition and parts by weight of the ignition raw materials are: 15 parts of potassium perchlorate, 8 parts of antimony sulfide, 3 parts of aluminum powder, 0.5 part of barium nitrate, 0.8 part of manganese dioxide, and 2 parts of gum.
[0023] The production method is as follows:
[0024] (1) Melt the gum in hot water heated to 80°C until it becomes gelatinous, and set aside.
[0025] (2) 15 parts of potassium perchlorate, 8 parts of antimony sulfide, 3 parts of aluminum powder, 0.5 part of barium nitrate, and 0.8 part of manganes...
Embodiment 2
[0031] The formula and production method of embodiment 2 mixing flammable incense
[0032] formula:
[0033] The weight ratio of the ignition material to the main material of the incense is 1:99.
[0034] The composition and parts by weight of the main raw materials for burning incense are: 20 parts of wood powder, 20 parts of pine bark powder, 1 part of laurel leaf powder, 1 part of scarlet pigment and 3 parts of rosin.
[0035] The composition and parts by weight of the ignition raw materials are: 30 parts of potassium perchlorate, 15 parts of antimony sulfide, 8 parts of aluminum powder, 2 parts of barium nitrate, 1.5 parts of manganese dioxide, and 3 parts of polyvinyl alcohol.
[0036] The production method is as follows:
[0037] (1) Melt polyvinyl alcohol in hot water heated to 75°C until it becomes gelatinous, and set aside.
[0038] (2) 30 parts of potassium perchlorate, 15 parts of antimony sulfide, 8 parts of aluminum powder, 2 parts of barium nitrate, 1.5 part...
Embodiment 3
[0044] The formula and production method of embodiment 3 mixed combustible incense
[0045] formula:
[0046] The weight ratio of the ignition raw material to the incense main raw material is 1:20.
[0047] The composition and parts by weight of the main raw materials for burning incense are: 20 parts of wood powder, 10 parts of ginkgo bark powder, 0.5 part of osmanthus leaf powder, 0.5 part of orange yellow pigment, and 2 parts of rosin.
[0048] Composition and parts by weight of the ignition raw materials are: 15 parts of potassium perchlorate, 8 parts of antimony sulfide, 3 parts of aluminum powder, 0.5 part of barium nitrate, 0.8 part of manganese dioxide, 1 part of dextrin and 1 part of starch.
[0049] The production method is as follows:
[0050] (1) Melt the dextrin and starch in hot water heated to 85°C until it becomes gelatinous, and set aside.
[0051] (2) 15 parts of potassium perchlorate, 8 parts of antimony sulfide, 3 parts of aluminum powder, 0.5 part of ...
PUM
Property | Measurement | Unit |
---|---|---|
length | aaaaa | aaaaa |
diameter | aaaaa | aaaaa |
length | aaaaa | aaaaa |
Abstract
Description
Claims
Application Information
- R&D Engineer
- R&D Manager
- IP Professional
- Industry Leading Data Capabilities
- Powerful AI technology
- Patent DNA Extraction
Browse by: Latest US Patents, China's latest patents, Technical Efficacy Thesaurus, Application Domain, Technology Topic, Popular Technical Reports.
© 2024 PatSnap. All rights reserved.Legal|Privacy policy|Modern Slavery Act Transparency Statement|Sitemap|About US| Contact US: help@patsnap.com